微型化LD泵浦Er3+,Yb3+共掺磷酸盐玻璃被动调Q激光器

上一篇

下一篇

郭猛, 惠勇凌, 王万祎, 姜梦华, 雷訇, 李强. 2014: 微型化LD泵浦Er3+,Yb3+共掺磷酸盐玻璃被动调Q激光器, 强激光与粒子束, 26(9): 7-11. doi: 10.11884/HPLPB201426.091001
引用本文: 郭猛, 惠勇凌, 王万祎, 姜梦华, 雷訇, 李强. 2014: 微型化LD泵浦Er3+,Yb3+共掺磷酸盐玻璃被动调Q激光器, 强激光与粒子束, 26(9): 7-11. doi: 10.11884/HPLPB201426.091001
Guo Meng, Hui Yongling, Wang Wanyi, Jiang Menghua, Lei Hong, Li Qiang. 2014: Miniature LD pumped passively Q-switched Er3+ ,Yb3+ co-doped phosphate glass laser, High Power Lase and Particle Beams, 26(9): 7-11. doi: 10.11884/HPLPB201426.091001
Citation: Guo Meng, Hui Yongling, Wang Wanyi, Jiang Menghua, Lei Hong, Li Qiang. 2014: Miniature LD pumped passively Q-switched Er3+ ,Yb3+ co-doped phosphate glass laser, High Power Lase and Particle Beams, 26(9): 7-11. doi: 10.11884/HPLPB201426.091001

微型化LD泵浦Er3+,Yb3+共掺磷酸盐玻璃被动调Q激光器

Miniature LD pumped passively Q-switched Er3+ ,Yb3+ co-doped phosphate glass laser

  • 摘要: 报道了一种主要应用于激光测距的微型化激光二极管泵浦Er3+/Yb3+共掺磷酸盐玻璃被动调Q激光器.采用中心波长940 nm的二极管作为泵浦源,Er3+/Yb3+共掺磷酸盐玻璃作为增益介质,Co2+:MgAl2O4作为被动调Q晶体,通过优化增益介质和被动调Q晶体参数,获得了最佳的增益介质长度和被动调Q晶体初始透过率.当泵浦能量14 mJ,重复频率10 Hz,泵浦脉宽5 ms时,获得了单脉冲能量480 μJ,脉宽5ns,峰值功率大于20 kW的激光输出,激光光束质量因子为1.2.
  • 加载中
  • 加载中
计量
  • 文章访问数:  352
  • HTML全文浏览数:  94
  • PDF下载数:  22
  • 施引文献:  0
出版历程
  • 刊出日期:  2014-09-30

微型化LD泵浦Er3+,Yb3+共掺磷酸盐玻璃被动调Q激光器

  • 北京工业大学激光工程研究院,北京,100124

摘要: 报道了一种主要应用于激光测距的微型化激光二极管泵浦Er3+/Yb3+共掺磷酸盐玻璃被动调Q激光器.采用中心波长940 nm的二极管作为泵浦源,Er3+/Yb3+共掺磷酸盐玻璃作为增益介质,Co2+:MgAl2O4作为被动调Q晶体,通过优化增益介质和被动调Q晶体参数,获得了最佳的增益介质长度和被动调Q晶体初始透过率.当泵浦能量14 mJ,重复频率10 Hz,泵浦脉宽5 ms时,获得了单脉冲能量480 μJ,脉宽5ns,峰值功率大于20 kW的激光输出,激光光束质量因子为1.2.