气相/凝聚炸药爆轰合成的碳包铜纳米颗粒特征

上一篇

下一篇

闫鸿浩, 张潇飞, 赵碧波, 赵铁军, 李晓杰. 2017: 气相/凝聚炸药爆轰合成的碳包铜纳米颗粒特征, 强激光与粒子束, 29(8): 70-74. doi: 10.11884/HPLPB201729.170074
引用本文: 闫鸿浩, 张潇飞, 赵碧波, 赵铁军, 李晓杰. 2017: 气相/凝聚炸药爆轰合成的碳包铜纳米颗粒特征, 强激光与粒子束, 29(8): 70-74. doi: 10.11884/HPLPB201729.170074
Yan Honghao, Zhang Xiaofei, Zhao Bibo, Zhao Tiejun, Li Xiaojie. 2017: Characteristics of carbon encapsulated copper nanoparticles based on gaseous/condensed explosives detonation, High Power Lase and Particle Beams, 29(8): 70-74. doi: 10.11884/HPLPB201729.170074
Citation: Yan Honghao, Zhang Xiaofei, Zhao Bibo, Zhao Tiejun, Li Xiaojie. 2017: Characteristics of carbon encapsulated copper nanoparticles based on gaseous/condensed explosives detonation, High Power Lase and Particle Beams, 29(8): 70-74. doi: 10.11884/HPLPB201729.170074

气相/凝聚炸药爆轰合成的碳包铜纳米颗粒特征

Characteristics of carbon encapsulated copper nanoparticles based on gaseous/condensed explosives detonation

  • 摘要: 采用凝聚炸药爆轰和气相爆轰分别制备碳包铜纳米颗粒,并利用XRD,Raman和TEM等方法对合成纳米产物进行对比分析.其中凝聚炸药爆轰法以柠檬酸铜干凝胶、油酸和黑索金为原料按照一定比例配成爆炸源,在氮气的保护氛围中引爆;而气相爆轰法以乙酰丙酮铜为原料,分别以H2和O2,H2和空气为爆炸源,在负氧条件下引爆.通过XRD,Raman和TEM分析结果表明,两类爆轰法均可得到分散性良好的碳包覆铜纳米颗粒,碳壳石墨化程度较高.气相爆轰可以合成10 nm以下的纳米晶粒,而凝聚炸药爆轰合成的晶粒尺寸在20~40 nm,且存在较多空壳结构;气相爆轰产物其碳壳尺寸在2~3 nm,凝聚炸药爆轰产物其碳壳尺寸在2~5 nm.
  • 加载中
  • 加载中
计量
  • 文章访问数:  374
  • HTML全文浏览数:  201
  • PDF下载数:  14
  • 施引文献:  0
出版历程
  • 刊出日期:  2017-08-30

气相/凝聚炸药爆轰合成的碳包铜纳米颗粒特征

  • 大连理工大学 工程力学系,辽宁 大连,116023

摘要: 采用凝聚炸药爆轰和气相爆轰分别制备碳包铜纳米颗粒,并利用XRD,Raman和TEM等方法对合成纳米产物进行对比分析.其中凝聚炸药爆轰法以柠檬酸铜干凝胶、油酸和黑索金为原料按照一定比例配成爆炸源,在氮气的保护氛围中引爆;而气相爆轰法以乙酰丙酮铜为原料,分别以H2和O2,H2和空气为爆炸源,在负氧条件下引爆.通过XRD,Raman和TEM分析结果表明,两类爆轰法均可得到分散性良好的碳包覆铜纳米颗粒,碳壳石墨化程度较高.气相爆轰可以合成10 nm以下的纳米晶粒,而凝聚炸药爆轰合成的晶粒尺寸在20~40 nm,且存在较多空壳结构;气相爆轰产物其碳壳尺寸在2~3 nm,凝聚炸药爆轰产物其碳壳尺寸在2~5 nm.