溶胶-凝胶法制备的纳米TiO2结构相变及晶体生长动力学

上一篇

下一篇

胡林华, 戴松元, 王孔嘉. 2003: 溶胶-凝胶法制备的纳米TiO2结构相变及晶体生长动力学, 物理学报, 52(9): 2135-2139. doi: 10.3321/j.issn:1000-3290.2003.09.007
引用本文: 胡林华, 戴松元, 王孔嘉. 2003: 溶胶-凝胶法制备的纳米TiO2结构相变及晶体生长动力学, 物理学报, 52(9): 2135-2139. doi: 10.3321/j.issn:1000-3290.2003.09.007
2003: Structural transformation of nanocrystalline titania grown by sol-gel technique and the growth kinetics of crystallites, Acta Physica Sinica, 52(9): 2135-2139. doi: 10.3321/j.issn:1000-3290.2003.09.007
Citation: 2003: Structural transformation of nanocrystalline titania grown by sol-gel technique and the growth kinetics of crystallites, Acta Physica Sinica, 52(9): 2135-2139. doi: 10.3321/j.issn:1000-3290.2003.09.007

溶胶-凝胶法制备的纳米TiO2结构相变及晶体生长动力学

Structural transformation of nanocrystalline titania grown by sol-gel technique and the growth kinetics of crystallites

  • 摘要: 讨论了采用溶胶-凝胶法经由先驱物钛酸四异丙脂水解而制备的纳米TiO2粉末的结构相变,并讨论了该纳米粉末的生长动力学机理.结果表明,水解pH值为0.9,当高压釜热处理温度<503K时,粉末晶粒度增长较为缓慢,而当热处理温度>503K时,粉末粒度明显长大.应用相变理论计算出了纳米TiO2颗粒的两阶段的生长激活能,分别是18.5kJ/mol和59.7kJ/mol.XRD物相分析表明,高压釜热处理温度达到503K时,样品就开始发生锐钛矿到金红石相的结构相变,到543K就基本实现了这一结构相变,使得这一相变温度比其他文献中报道的又降低了许多.
  • 加载中
  • 加载中
计量
  • 文章访问数:  983
  • HTML全文浏览数:  81
  • PDF下载数:  296
  • 施引文献:  0
出版历程

溶胶-凝胶法制备的纳米TiO2结构相变及晶体生长动力学

  • 中国科学院等离子体物理研究所,合肥,230031

摘要: 讨论了采用溶胶-凝胶法经由先驱物钛酸四异丙脂水解而制备的纳米TiO2粉末的结构相变,并讨论了该纳米粉末的生长动力学机理.结果表明,水解pH值为0.9,当高压釜热处理温度<503K时,粉末晶粒度增长较为缓慢,而当热处理温度>503K时,粉末粒度明显长大.应用相变理论计算出了纳米TiO2颗粒的两阶段的生长激活能,分别是18.5kJ/mol和59.7kJ/mol.XRD物相分析表明,高压釜热处理温度达到503K时,样品就开始发生锐钛矿到金红石相的结构相变,到543K就基本实现了这一结构相变,使得这一相变温度比其他文献中报道的又降低了许多.