非晶Fe73.5Cu1Nb3Si13.5B9合金激光纳米化的超精细结构研究

上一篇

下一篇

陈岁元, 刘常升, 李慧莉, 崔彤. 2005: 非晶Fe73.5Cu1Nb3Si13.5B9合金激光纳米化的超精细结构研究, 物理学报, 54(9): 4157-4163. doi: 10.3321/j.issn:1000-3290.2005.09.036
引用本文: 陈岁元, 刘常升, 李慧莉, 崔彤. 2005: 非晶Fe73.5Cu1Nb3Si13.5B9合金激光纳米化的超精细结构研究, 物理学报, 54(9): 4157-4163. doi: 10.3321/j.issn:1000-3290.2005.09.036
CHEN Sui-yuan, Liu Chang-Sheng, LI Hui-li, Cui Tong. 2005: Hyperfine stucture during nanocrystallization of amorphous Fe73.5Cu1Nb3Si13.5B9 alloy irradiated by laser, Acta Physica Sinica, 54(9): 4157-4163. doi: 10.3321/j.issn:1000-3290.2005.09.036
Citation: CHEN Sui-yuan, Liu Chang-Sheng, LI Hui-li, Cui Tong. 2005: Hyperfine stucture during nanocrystallization of amorphous Fe73.5Cu1Nb3Si13.5B9 alloy irradiated by laser, Acta Physica Sinica, 54(9): 4157-4163. doi: 10.3321/j.issn:1000-3290.2005.09.036

非晶Fe73.5Cu1Nb3Si13.5B9合金激光纳米化的超精细结构研究

Hyperfine stucture during nanocrystallization of amorphous Fe73.5Cu1Nb3Si13.5B9 alloy irradiated by laser

  • 摘要: 在CO2激光功率为50-300W、扫描速度为20mm/s、激光散光斑为20mm照射条件下,诱导非晶Fe73.5Cu1Nb3Si13.5B9带中发生结构重组,产生定量纳米α-Fe(Si)晶相形成双相组织结构材料. 利用穆斯堡尔谱研究了非晶Fe73.5Cu1Nb3Si13.5B9合金激光纳米化的超精细结构. 实验结果表明,激光诱导非晶Fe73.5Cu1Nb3Si13.5B9纳米化后,其超精细磁场的分布随着激光功率变化由单峰向双峰变化,在高功率辐照时, 出现了双峰分布,并且峰位向高场移动. 高激光功率辐照非晶Fe73.5Cu1Nb3Si13.5B9合金纳米晶化相有四种超精细结构,即2个超精细磁场较小的初晶相和2个超精细磁场较大的纳米晶化相. 其中超精细磁场较大(17-25MA/m)的α-Fe(Si)相为DO3结构.
  • 加载中
  • 加载中
计量
  • 文章访问数:  396
  • HTML全文浏览数:  71
  • PDF下载数:  47
  • 施引文献:  0
出版历程
  • 刊出日期:  2005-09-30

非晶Fe73.5Cu1Nb3Si13.5B9合金激光纳米化的超精细结构研究

  • 东北大学材料与冶金学院,沈阳,110004

摘要: 在CO2激光功率为50-300W、扫描速度为20mm/s、激光散光斑为20mm照射条件下,诱导非晶Fe73.5Cu1Nb3Si13.5B9带中发生结构重组,产生定量纳米α-Fe(Si)晶相形成双相组织结构材料. 利用穆斯堡尔谱研究了非晶Fe73.5Cu1Nb3Si13.5B9合金激光纳米化的超精细结构. 实验结果表明,激光诱导非晶Fe73.5Cu1Nb3Si13.5B9纳米化后,其超精细磁场的分布随着激光功率变化由单峰向双峰变化,在高功率辐照时, 出现了双峰分布,并且峰位向高场移动. 高激光功率辐照非晶Fe73.5Cu1Nb3Si13.5B9合金纳米晶化相有四种超精细结构,即2个超精细磁场较小的初晶相和2个超精细磁场较大的纳米晶化相. 其中超精细磁场较大(17-25MA/m)的α-Fe(Si)相为DO3结构.