Yb3+/Er3+共掺锗碲酸盐玻璃上转换发光增强机理的研究

上一篇

下一篇

杨中民, 张勤远, 刘粤惠, 姜中宏. 2005: Yb3+/Er3+共掺锗碲酸盐玻璃上转换发光增强机理的研究, 物理学报, 54(5): 2013-2018. doi: 10.3321/j.issn:1000-3290.2005.05.010
引用本文: 杨中民, 张勤远, 刘粤惠, 姜中宏. 2005: Yb3+/Er3+共掺锗碲酸盐玻璃上转换发光增强机理的研究, 物理学报, 54(5): 2013-2018. doi: 10.3321/j.issn:1000-3290.2005.05.010
Yang Zhong-Min, Zhang Qin-Yuan, Liu Yue-Hui, Jiang Zhong-Hong. 2005: Mechanism of the enhanced upconversion emissions in Yb3+/Er3 + -codoped germanate-tellurite glasses, Acta Physica Sinica, 54(5): 2013-2018. doi: 10.3321/j.issn:1000-3290.2005.05.010
Citation: Yang Zhong-Min, Zhang Qin-Yuan, Liu Yue-Hui, Jiang Zhong-Hong. 2005: Mechanism of the enhanced upconversion emissions in Yb3+/Er3 + -codoped germanate-tellurite glasses, Acta Physica Sinica, 54(5): 2013-2018. doi: 10.3321/j.issn:1000-3290.2005.05.010

Yb3+/Er3+共掺锗碲酸盐玻璃上转换发光增强机理的研究

Mechanism of the enhanced upconversion emissions in Yb3+/Er3 + -codoped germanate-tellurite glasses

  • 摘要: 玻璃的最大声子能量决定稀土离子的上转换发光强度,但本研究发现:Yb3+/Er3+共掺锗碲酸盐玻璃在980nmLD抽运下,上转换荧光强度随着BiO3对PbO的取代和碱金属离子半径的增大而明显增强.而Raman光谱显示基质玻璃的最大声子能量并不随Bi2O3对PbO的取代和碱金属离子半径的增大而变化,但玻璃的最大声子密度随着Bi2O3对PbO取代和碱金属离子半径的增大而降低.从玻璃无辐射跃迁概率的角度,通过分析表明,最大声子密度的降低是玻璃上转换发光强度增强的主要原因.
  • 加载中
  • 加载中
计量
  • 文章访问数:  699
  • HTML全文浏览数:  86
  • PDF下载数:  124
  • 施引文献:  0
出版历程
  • 刊出日期:  2005-05-30

Yb3+/Er3+共掺锗碲酸盐玻璃上转换发光增强机理的研究

  • 华南理工大学光通信材料研究所,特种功能材料制备新技术教育部重点实验室,广州,510641

摘要: 玻璃的最大声子能量决定稀土离子的上转换发光强度,但本研究发现:Yb3+/Er3+共掺锗碲酸盐玻璃在980nmLD抽运下,上转换荧光强度随着BiO3对PbO的取代和碱金属离子半径的增大而明显增强.而Raman光谱显示基质玻璃的最大声子能量并不随Bi2O3对PbO的取代和碱金属离子半径的增大而变化,但玻璃的最大声子密度随着Bi2O3对PbO取代和碱金属离子半径的增大而降低.从玻璃无辐射跃迁概率的角度,通过分析表明,最大声子密度的降低是玻璃上转换发光强度增强的主要原因.