STM and spectroscopy are highly regarded techniques in the surface science [1]. They provide atomically resolved information on the local density of states (LDOS) and reveal the structure of energy bands with high resolution. STM has become essential tools for investigating quantum phenomena, including unconventional superconductivity [2−5], charge ordering [6, 7], Chern insulating states [8], topological magnetism [9−11], and correlated electronic phases [12] in condensed matter physics. Recent advancements in STM have enabled the exploration of complex magnetic and electronic structures in non-collinear antiferromagnetic half-metals [13], revealing their distinct spin arrangements and band structures [14]. These materials are well-suited for STM investigations under strong magnetic fields and at low temperatures, allowing for the direct visualization of quantum phase transitions and electron correlations, which are crucial for developing quantum materials and spintronic applications [15, 16]. Similarly, two-dimensional magnetic materials, with their atomically smooth surfaces and intrinsic magnetism, provide an ideal platform for STM studies. By mapping spin textures and electronic states, STM helps uncover the interplay between magnetism and topological properties, thus advancing research in low-dimensional quantum systems [17, 18]. These studies are essential for understanding novel electronic states and their applications in quantum computing and spintronic devices. While numerous commercial and custom STM designs have been developed [19−22], high-field STM systems remain relatively rare, largely due to spatial constraints and the technical demands associated with high-field operation. Developing compact and robust STM systems capable of achieving atomic resolution under harsh conditions, including high magnetic fields and low temperatures, is critical for advancing research on these novel material systems. Overcoming several technical challenges is necessary to enable high-field STM capabilities.
One of the primary challenges is the limitation of space. Superconducting magnets are capable of generating magnetic fields as strong as 20 T. This is achieved with a bore diameter of 50 mm and a base temperature of 4.2 K [23]. To reach even lower base temperatures, variable temperature inserts (VTIs) can be utilized. These include a 1 K-pot-based VTI, which is capable of reaching 1.5 K [24, 25], a 3He refrigerator-based VTI [26], and a dilution refrigerator-based VTI [27]. However, it should be noted that when a VTI is inserted into the magnet bore, the usable sample space is significantly reduced from 50 mm to 30 mm [28]. This reduction poses a constraint for the experimental setup and can impact the feasibility of certain experiments. As a result, high-field STMs operating at low temperatures are commonly situated in wet superconducting magnets. In this configuration, the coils are immersed in liquid helium to preserve their superconducting state. This arrangement offers a stable and low-vibration environment. However, it necessitates a substantial amount of liquid helium, and the recovery, purification, and reuse processes of helium are both time-consuming and labor-intensive. Conversely, the development of cryogen-free magnets has introduced an alternative, which employs a closed-loop helium expansion cycle to maintain the magnet coil at low temperatures. This innovation simplifies maintenance and operation. Despite this advantage, cryogen-free systems depend on a cryocooler, which generates considerable vibrations during operation, thereby potentially compromising the atomically resolved imaging capabilities of the STM. Consequently, the design of a STM intended for use in a cryogen-free magnet system faces considerable challenges. These challenges arise from the strict requirements for vibration resistance and the necessity for structural rigidity to reduce external disturbances. Ensuring that the STM can operate effectively under these conditions is a complex task, as the system must be robust enough to maintain stability despite potential external vibrations. Therefore, a high-field STM must be compact, rigid, and stable enough to resist external vibrations.
Recently, our research team has developed and built a series of STMs capable of high-resolution imaging under challenging conditions, including strong magnetic fields [24, 29−31] and low-temperature environments [32, 33]. Previous work by Meng et al. [29] demonstrated atomic-resolution imaging using STM inside a cryogen-free superconducting magnet. The STM design in their study primarily featured two PTs: one for coarse approach and the other for sample scanning. The operation of this system relies on a stick-slip mechanism combined with a double-slider push structure. This design introduces challenges related to achieving high processing precision and maintaining the coaxial alignment. The complexity of maintaining such precision is due to the inherent intricacies of the stick-slip motion, which requires careful control to avoid deviations. To overcome these issues, Wang et al. [24] developed an STM head with a standalone scanner configuration, also using two PTs. However, unlike earlier models, the scanner disengages from the longer PT after the coarse approach. While the design of this STM is optimized for narrow spaces, its lateral dimensions restrict its ability to rotate within small-bore magnets. In response to these challenges, Geng et al. [33] developed a compact STM designed to operate within a cryogen-free superconducting magnet. This design incorporates a single tantalum shaft with coaxially nested PTs. Although this configuration reduces the spatial footprint, it introduces complexity to the STM head structure, adversely affecting its rigidity and imaging stability. Moreover, the study highlighted the risk of tip-to-sample collisions, attributed to the high pulse signals used during shaft retraction at low temperatures.
To address the previously highlighted challenges, a miniature inertial piezoelectric motor with a highly compact design has been developed in this study. This motor features a small PT scanner and a PS secured by a CuBe spring strip, resulting in an ultra-compact STM enable to work in high magnetic field and at low temperature. This design effectively addresses key issues inherent to inertial piezoelectric motors, enhancing the stability and precision of the STM. Its low threshold voltage under ambient conditions has enabled testing in challenging environments, including high magnetic fields and low temperatures. Significantly, the PS is utilized as a coarse approach inside the scanning tube for the first time in STM technology within a cryogen-free superconducting magnet. The device boasts an impressively low eigenfrequency of 20 kHz [34], which substantially improves its resistance to external mechanical and acoustic disturbances. Furthermore, the STM’s excellent insulating properties effectively shield it from magnetic field ripples, preventing eddy current coupling and reducing temperature instability caused by eddy current heating during field enhancement. The long-term stability of the STM is confirmed by the low drift rates in both the X-Y plane and Z-direction at low temperature. Additionally, the STM’s performance has been validated through atomic-resolution imaging of graphite and NbSe2 at low temperatures under magnetic fields ranging from 0 to 9 T. With its compact dimensions of 9 mm in width and 22 mm in length, this STM head shows significant promise for the development of a rotatable STM, similar to the piezoelectric rotatable magnetic force microscope (MFM) [35].
-
The STM head consists of several components, including a single PT, PS, a spring strip, a tantalum weight, a sapphire main body, and a bottom cover. FIG. 1(a, b) shows a sectional and an exploded view which illustrate the overall structure of the STM head unit. Compared to other reported STM designs, our STM head is significantly smaller, with a length of only 22 mm and a diameter of 9 mm, as shown in FIG. 1(c). The coarse-approach mechanism and scanning function are driven by a small PT (EBL#3, 0.5 mm thickness, with a 3.30 mm outer diameter and 9 mm length, from EBL Products Inc.) and a PS (1.1 mm thickness, 1.95 mm width, and 13 mm length), which move the sample toward the tip. A support spring strip clamps the PS at the free end of the PT, allowing smooth vertical movement along the tube’s inner wall. The structure of this PT-based inertial motor, its working principle, performance, and application in atomic imaging under ambient conditions were detailed in our previous work [34]. Due to its low threshold voltage in ambient conditions, it has been tested under extreme environments, such as high magnetic fields and low temperatures. Notably, the piezoelectric shaft, functioning as a scanner, is being used for the first time in STM technology within a cryogen-free superconducting magnet. The PS and Piezo tube (PT) can expand and contract independently. In contrast, metallic or zirconium shafts do not expand. This independence allows the PS to respond to the applied voltage by expanding and contracting as needed, helping to precisely control the distance between the tip and the sample. It is important to note that when a small PT functions as a piezoelectric motor (PM), it may not generate enough inertial force for precise step-by-step shaft movement due to its limited expansion. However, by integrating the PS with the small PT for the first time, we successfully resolved this issue, enabling precise control of the distance between the tip and the sample. The use of sapphire components ensures that the STM head remains non-magnetic, allowing it to operate reliably in high magnetic fields. The sample is glued to one side of the PS. The tip holder, also made of sapphire, securely holds the Pt/Ir tip used for measurements. The tip, made from a Pt/Ir alloy (90:10), is cut at an angle of 15° to 30° using scissors. Silver conductive paint is used to secure both the tip and the sample in place.
-
This system is a low-temperature, liquid-helium-free superconducting magnet system manufactured by Oxford Instruments. An STM rod was inserted through a KF50 quick flange into the magnet’s variable temperature insert (VTI) within the sample space, which has a central tube with a 50 mm diameter. The VTI features an independent helium circulation loop and a sealed gas handling system, including a small storage container and a mechanical pump. This setup circulates helium to regulate and maintain the desired temperature. Inside the VTI, a heat exchanger with a temperature sensor and a heater ensures stable temperatures, controlled by a PID feedback system. The sample compartment is filled with static helium exchange gas, allowing efficient thermal exchange with the VTI’s heat exchanger, thereby maintaining the sample and STM head temperatures between 1.6 K and 300 K. The magnet’s superconducting coil is cooled by a cryostat positioned below the sample chamber. When the probe was inserted, the STM head was precisely centered within the magnet coil which generated adjustable magnetic fields ranging from 0 to 9 T. FIG. 2 (a) and (b) present a photograph and a schematic of the experimental system, respectively. The rod comprised an aluminum preamplifier circuit box, a KF50 flange, a bellows joint, a central stainless-steel pipe (304-grade), three stainless steel radiation shield plates, a balancing weight, a spacing ring, a multi-pin sapphire interface piece, a vibration isolation spring, an enclosure, and the STM head. The preamplifier circuit box, attached to the upper end of the central tube through a bellows joint, contained a specially designed STM preamplifier circuit with a 100 MΩ feedback resistor and a 200 Hz bandwidth. A custom electrical feedthrough between the KF50 flange and the preamplifier box ensured signal transmission while maintaining the vacuum seal of the sample chamber, as noted in the reference [33]. Notably, the preamplifier circuit box was the only component located outside the magnetic sample chamber, while all other components remained inside. To accommodate the lightweight design of the sapphire STM body, the signal cables connecting it to the terminal consisted of 0.07 mm diameter enameled silver wire. A cover mounted on the terminal prevented the wires from contacting the inner walls of the sample portion, effectively reducing interference. A Teflon circular piece was placed at the base of the probe in our STM rod to align it coaxially with the magnet’s aperture. The probe employed a secondary passive vibration isolation system to minimize vibrations. In the first stage, soft welded bellows were attached to the top of the central rod, with a balancing weight of alternating Teflon and brass cylinders below to lower the resonant frequency and reduce thermal transfer. This design prevented thermal short circuits within the magnet’s cold sections due to the mass and size of the brass blocks. In the second stage, a vibration isolation spring made of 0.15 mm CuBe wire, with a diameter of 3.5 mm and a length of 90 mm, supported the STM head just below the terminal, thus achieving an eigenfrequency of around 2 Hz. The STM rod was securely attached to the magnet with a KF50 flange, using a plastic clamp and polymer gasket for electrical isolation. The STM head and rod were grounded through a dedicated wire connected to a thick copper pillar embedded in the ground, independent of the magnet system’s ground, to reduce electromagnetic interference. The STM controller in our setup was custom-built, based on a National Instruments (NI) PXI-7851R data acquisition card. This setup allowed for coarse approach, scanning, imaging, and data collection, all controlled by a custom LabVIEW program accessible online. The controller and power module were placed 1.5 meters away from the magnetic field to prevent interference.
-
Our STM probe rod could be easily inserted into the liquid helium-free superconducting magnet for measurements and quickly removed once the measurements were completed, allowing the magnet to be available for other experiments. It was important to ensure that the magnet’s sample chamber remained under positive pressure when inserting or removing the STM probe rod to prevent outside air from entering and causing ice formation in the low-temperature chamber. After removing the STM probe rod, the sample chamber of the magnet was cleaned with helium two to three times before being pumped out. During experiments, the tip was grounded, and a virtual signal was applied to the biased sample through the inverting input of the first stage of an operational amplifier. At 300 K, STM images were continuously captured while the magnetic field varied from 0 T to 9 T, as shown in FIG. 3. This STM, featuring a shaft made entirely of piezo material, is the first time to operate within a cryogen-free superconducting magnet. The STM maintained excellent imaging quality throughout the full range of magnetic field variations. As the magnetic field increases, significant changes in the local density of states (LDOS) and the periodicity of the atomic lattice are observed in the atomic-resolution images. These images provide direct evidence of field-induced modifications, reinforcing the idea that magnetic fields influence the atomic-scale properties of materials. The high-quality imaging achieved within the magnet further demonstrated the STM’s stability and precision.
To assess the effectiveness of the STM body at decreasing temperatures, the sample area was cooled to 1.8 K by adjusting the VTI needle valve flow. Atomic resolution images of the graphite surface were subsequently acquired at 1.8 K under 0 T and 9 T magnetic fields, as presented in FIG. 4. Notably, the piezoelectric coefficient of piezoelectric materials significantly diminishes at temperatures below 4 K. Consequently, the driving capability of piezoelectric motors is also considerably reduced at low temperatures. Despite this, our motor continued to operate effectively under these conditions. A driving voltage of 180 V was applied to power the motor, and the slider consistently overcame gravitational forces to step upward.
We also examined a single crystal of NbSe2 to evaluate the STM’s capabilities on dynamic samples, given that NbSe2 has a superconducting transition temperature (Tc) close to 7 K. FIG. 5(a) shows atomic-resolution images of NbSe2 captured in constant height mode at low temperature. Due to NbSe2’s susceptibility to oxidation in air, it is essential to cleave a fresh surface quickly. Typically, the sample was cleaved within a minute before inserting the STM into the cryostat, minimizing the risk of surface degradation during imaging. The stability of a low-temperature STM is closely linked to the performance of STS measurements. FIG. 5(b) shows high-resolution
$\dfrac{{\rm{d}}I}{{\rm{d}}V}$ spectra of NbSe2, obtained as the temperature of 3 K and 8 K. The$\dfrac{{\rm{d}}I}{{\rm{d}}V}$ spectra reveal the dynamic evolution of the superconducting gap in NbSe2 as the temperature decreases from 8 K to 3 K, in agreement with previously reported findings. As shown in FIG. 5(b), the black line shows that the superconducting gap of NbSe2 does not appear when the temperature is at 8 K, but red lines become evident with a width below 3 mV when the temperature drops to 7 K, and it continues to sharpen as the temperature decreases to 3 K. The atomic-resolution images of NbSe2 remained exceptionally stable, highlighting the STM’s remarkable resistance to both low temperature and external vibrations.Achieving high-resolution imaging relies on the compact and rigid design of the STM head. The long-term stability of our STM was evaluated by drift measurements taken over 60 min, as shown in FIG. 6. The tunneling current was set to 1 nA, with a bias voltage of 100 mV and the tip grounded. Average drift rates were calculated through linear regression, showing 3.5 pm/min in the X-Y plane and 4.1 pm/min along the Z-axis at 1.8 K. The long-term stability of the STM is indicated by these low drift rates. The system exhibited exceptionally low drift despite the STM rod being directly attached to the cryostat.
-
In conclusion, this study presented the development of an innovative STM integrated with a cryogen-free superconducting magnet. The design featured a streamlined and ultra-compact STM head, which was specifically engineered to fit within narrow sample spaces. This ensured that the tip-sample loop remained compact and unaffected by the coarse approach motor. High-resolution atomic images of the highly oriented pyrolytic graphite (HOPG) surface were captured at 1.8 K in magnetic fields ranging from 0 to 9 T, demonstrating the STM’s stability and robustness in both low-temperature and high-field environments. Additionally, atomic-resolution imaging of the NbSe2 surface and dI/dV spectra of NbSe2 at 3 K further validated the STM’s exceptional capabilities for high-resolution imaging. The STM head’s short axial length offered significant potential for integration into a rotatable STM system. By enabling STM rotation, researchers could conduct a more comprehensive analysis of material properties under varying magnetic field orientations, which is crucial for advancing the understanding of two-dimensional materials.
Integrating STM with Cryogen-Free Systems for Enhanced Stability in Harsh Conditions
- Received Date: 13/01/2025
- Available Online: 27/10/2026
-
Key words:
- Scanning tunneling microscopy /
- Piezoelectric shaft /
- High magnetic field /
- Cryogen free superconducting magnet /
- Low temperature
Abstract: Scanning tunneling microscopy (STM) achieves atomic-level imaging, which is vital in the advancements of physics and materials science. Conducting spectroscopy and imaging at low temperatures with magnetic fields is complex, further complicated in cryogen-free systems by noise and vibrations from cryogenic equipment. We successfully integrated a compact STM with a cryogen-free superconducting magnet. The STM head features a simple design with a single piezoelectric tube (PT) and a piezoelectric shaft (PS) secured by a CuBe spring strip. The PS is used as a coarse approach mechanism inside the scanning tube and integrated with a cryogen-free superconducting magnet. STM long term stability were confirmed by achieving minimal drift rates of 3.5 pm/min in the X-Y plane and 4.1 pm/min along the Z-axis at 1.8 K. Experiments were also conducted with magnetic fields ranging from 0 T to 9 T at 300 K, which yielded high-quality atomic-resolution images of graphite sample. Additionally, the atomic-resolution imaging and