The use of fossil fuels has not only facilitated the rapid development of human society and the economy but also led to a large amount of environmental pollution and ecological problems, resulting in a great crisis for human survival [1, 2]. In addition, the combustion of fossil fuels produces a large amount of CO2, which is considered as the main cause of the greenhouse effect. Therefore, reducing emissions and effectively utilizing CO2 are important challenges that urgently need to be solved [3, 4]. Currently, CO2 capture and storage, CO2 hydrogenation conversion, and CO2 recycling have been widely developed to solve this crisis [5, 6]. The catalytic hydrogenation of CO2 can generate chemical industrial raw materials and chemical fuels, and is widely used in the agricultural field. It is considered one of the most promising technologies for alleviating the CO2 crisis [7, 8].
CO2 molecules have good thermal stability, and many parallel reactions occur during the hydrogenation reaction; thus, the reaction products are dispersed and difficult to control [9, 10]. For example, the hydrogenation products of CO2 include acid derivatives, alcohol derivatives, hydrocarbon derivatives, and CO. Therefore, it is still challenging to effectively activate thermodynamically stable CO2 molecules to generate highly selective target products and reduce unnecessary side reactions [11, 12]. Among the numerous hydrogenation processes, CO2 hydrogenation to produce CO and CH4 products is the most common type of reaction, which are referred to as reverse water gas reactions and CO2 methanation, respectively [13, 14]. Recently, the rapid development of heterogeneous catalysts has effectively supported technological development to solve the CO2 crisis. This occurred because the different metal sites in heterogeneous catalysts; the structure of alloy catalysts, the type of support, the size of metal particles, the formation of special interfaces, and the design of composite catalysts may all effectively regulate CO2 hydrogenation [15−17]. In addition, Zhang et al. prepared a series of CoFe-based catalysts through hydrogen reduction of CoFeAl-LDH (LDH: layered double hydroxide) nanosheets. CoFe-based catalysts showed a progressive selectivity shift from CO to CH4 during CO2 hydrogenation. Various characterization and theoretical calculations showed that oxide-decorated CoFe-alloy nanoparticles weaken the adsorption characteristics of reaction intermediates, resulting in high product selectivity [18].
Ion-modified metal-based catalysts have also attracted extensive attention because of their excellent ability to regulate CO2 hydrogenation [19, 20]. Recently, Sun et al. reported that Cs+-modified Ag/C catalysts significantly increased the conversion efficiency of CO2 and the selectivity of CO products. Various characterization results and theoretical simulation results revealed that the modification of Cs+ ions facilitated the adsorption and desorption properties of the intermediates
$ ^*{\rm CO}_2 $ and$ ^*{\rm OH} $ , resulting in high yields of CO products under photocatalytic conditions [21]. In addition, Zhu et al. reported that surface modification of K+ ions on CoPc/CNT mixed catalysts could regulate the selectivity and yield of methanol [22]. Qin et al. elucidated the important regulatory role and intrinsic mechanism of metal cations in the initial activation stage of CO2 electrocatalytic reduction through advanced molecular dynamics simulations; they reported that cations could significantly reduce the energy barrier for CO2 adsorption and reduction on Au surfaces, which was conducive to the formation of key intermediates through inner layer electron transfer, regulating the conversion processes of CO2 [23]. Unlike the extensive research on the regulation of CO2 hydrogenation by metal cation modification, the differences in performance and essential mechanisms of anion-modified metal-based catalysts in regulating CO2 hydrogenation still require further discussion.In this work, we report the complete transformation of CO2 hydrogenation products from CO to CH4 over Ru/TiO2 catalysts was achieved by the modification of PO43− anions. Multiple characterization and theoretical simulation results have shown that PO43− anions mainly adsorb on Ru metal sites of the Ru/TiO2 catalyst surface, affecting the surface electronic properties of Ru sites and regulating the conversion efficiency of CO2. The CO temperature-programmed desorption (CO-TPD) characterization and diffuse reflectance infrared Fourier transform spectroscopy (DRIFTS) results of CO adsorption indicated that the Ru sites modified with PO43− anions improve the adsorption properties for CO intermediates, which is beneficial for obtaining highly selective CH4 products. Our work reveals the action mechanism of Ru/TiO2 catalysts modified by PO43− anions and their ability to induce CO2 hydrogenation. Compared with other modified Ru/TiO2 catalysts, the Ru/TiO2-3 catalyst not only achieves complete conversion of hydrogenation products but also increases the conversion efficiency of CO2 (Table S1 in Supplementary materials, SM), which provides a new direction for the synthesis of high-yield and specific CO2 hydrogenation products.
-
High-purity ruthenium chloride (RuCl3·xH2O, Ru content 45%−55%), anatase titanium dioxide (TiO2, 99.8%, 25 nm), decalin (AR), sodium phosphate (Na3PO4, purity ≥99%), sodium chloride (NaCl, purity ≥99%), and sodium nitrate (NaNO3, purity ≥99%) were purchased from Aladdin Chemical Reagent Co. Ltd.
-
First, 0.5 g of TiO2 powder was added to a round bottom flask containing 95 mL of ultrapure water, and the flask was then placed in an oil bath and stirred at 50 °C. Second, 1.6 mL of RuCl3 solution (0.03 mol/L) and sodium phosphate were added to the flask and stirred for 12 h. Third, the aforementioned samples were filtered and washed with 200 mL of ultrapure water, and the obtained solid was dried in a vacuum oven at 80 °C. Last, the dried sample was ground and then calcined in a H2 atmosphere at 300 °C for 2 h to obtain the PO43−-modified Ru/TiO2-x catalyst. Ru/TiO2 catalysts modified with different contents of PO43− anions were synthesized by controlling the molar amount of sodium phosphate added during preparation (0.003, 0.002, 0.001, and 0 mol), which were represented as the Ru/TiO2-3, Ru/TiO2-2, Ru/TiO2-1, and Ru/TiO2-0 catalysts, respectively.
The Ru/TiO2 catalyst modified with 0.003 mol of PO43− anions without the H2 reduction step at 300 °C was named pre-Ru/TiO2-3.
For comparison, the Ru/TiO2 catalysts modified with 0.003 mol of Cl− or NO3− anions were prepared using the similar method by replacing sodium phosphate with sodium chloride or sodium nitrate, which were designated as Ru/TiO2-Cl or Ru/TiO2-N, respectively.
-
Inductively coupled plasma-optical emission spectrometer (ICP-OES) was obtained by thermal sensitive iCAP6300 spectrometer to analyze the actual Ru metal content in different Ru/TiO2 catalysts. X-ray diffraction (XRD) patterns were obtained by Cu Kα radiation on Miniflex II diffractometer. Transmission electron microscope (TEM) images and high resolution (HR-TEM) images were obtained by JEM-2010F instrument. The X-ray photoelectron spectroscopy (XPS) of elements in the catalyst was recorded by ESCALAB 250 spectrometer, and the binding energy of the catalysts were calibrated according to the peak value (284.6 eV) of C 1s. The specific surface area of samples was measured through Brunauer-Emmett-Teller (BET) method from the data with P/P0 ranging from 0.05 to 0.2.
The concentrations of PO43− anions on the different Ru/TiO2 catalyst surfaces were determined through Metrohm IC-940 ion chromatography, and the test steps were as follows: First, the initial concentration of PO43− anions in the sodium phosphate added during the preparation step of the Ru/TiO2 catalysts was measured. Second, the content of PO43− anions in the filtrate after filtration was determined. Last, the content of PO43− anions on the different Ru/TiO2 catalyst surfaces was determined by calculating the difference between the above two contents.
The CO temperature-programmed desorption (CO-TPD) spectra of the different catalysts were obtained by a TP-5080 instrument, and the detailed test steps were as follows: First, 100 mg of catalyst was weighed and pretreated in a H2 atmosphere at 300 °C for 1 h, then cooled to 50 °C for CO adsorption. Second, after CO was adsorbed for 20 min, the catalyst was purged with Ar gas for 30 min to remove physically adsorbed CO. Last, the desorption spectrum was recorded in the temperature range of 50 °C to 600 °C (the heating rate was 10 °C·min−1).
In situ diffuse reflectance infrared Fourier transform spectroscopy (in situ DRIFTS) was performed using a Bruker tensor II spectrometer, and the detailed test steps were as follows: First, a specific amount of catalyst was weighed and placed in the in situ cell. Second, Ar was introduced into the in situ cell, and the cell was heated to 200 °C for 1 h to remove surface moisture. When the temperature of the in situ cell cooled to 50 °C, the background spectrum was recorded. The in situ cell was subsequently heated to 300 °C, the Ar was replaced with a H2/CO2 mixture, and the reaction spectra were recorded. The CO adsorption spectrum of the catalyst were recorded through similar steps.
-
The catalytic performance of different Ru/TiO2 catalysts was evaluated in a 100 mL stainless steel autoclave, and the detailed test steps were as follows: First, 100 mg of catalyst and 10 mL of decalin solution were added to the autoclave. and then the reaction gas (H2/CO2 = 3:1) was introduced for 2 min to purge the air in the autoclave. Second, the pressure in the autoclave was 1 MPa, and the temperature was 300 or 200 °C. The reaction time was 1.5 h. After the reaction, the reaction autoclave was placed in a water bath to cool. The reactant conversion and product selectivity were analyzed by gas chromatography on a GC-2014 instrument. The detailed calculation formulas are as follows:
Conv.(CO2) and Sel.(CH4 or CO) represent the CO2 conversion and selectivity of CH4 or CO, respectively.
$M_{\text{CO}_2}$ and$ M_{\text{CO}_2}' $ represent the mole of CO2 before the reaction and after the reaction, respectively.$ M_{\text{CH}_4}' $ or$ M'_{\text{CO}} $ represents the mole of CH4 or CO after the reaction.During the catalyst cycle test, the used catalyst was washed by filtration and dried in an oven at 80 °C for further use. The detailed procedure was as follows: After the stainless steel autoclave was cooled to room temperature, the reaction solution from the autoclave was poured into a filtration bottle, and the autoclave was washed multiple times with methanol to ensure that all the catalyst was poured into the filtration bottle, after which the filtration process was performed. The collected catalyst was dried in an oven at 80 °C overnight, and then the next catalytic experiment was performed.
-
The spin polarization density function was calculated by the Vienna ab initio simulation software package (VASP) through the Perdew–Burke–Ernzerhof (PBE) exchange–correlation function [24, 25]. The DFT-D3 functional considers weak van der Waals interactions and sets the cut-off energy of the plane wave to 400 eV. After the geometric model was optimized, the force threshold on each atom was reduced to 0.05 eV/Å, and the total energy of the system was reduced to 10−5 eV. The gamma points in the Brillouin zone were selected for integration. The TiO2(101) surface was constructed by a 3 × 4 supercell with dimensions of 16.33 Å × 15.10 Å × 20.84 Å. The Ru clusters contained 16 atoms, and their arrangement was similar to that of the hexagonal close-packed (hcp) structure.
-
The physicochemical and structural properties of different Ru/TiO2 catalysts were investigated through multiple characterizations and theoretical calculations. First, the content of PO43− anions on different Ru/TiO2 catalyst surfaces was determined by comparing the difference between the total amount of PO43− anions added during catalyst preparation and the content of PO43− anions in the filtrate. As shown in Table S2 (SM), the concentrations of PO43− anions on the surface of the Ru/TiO2-0, Ru/TiO2-1, Ru/TiO2-2, and Ru/TiO2-3 catalysts increased to 0, 0.08, 0.23, and 0.29 mmol/gcat, respectively, indicating that Ru/TiO2 catalysts modified with different PO43− anion contents could be obtained by adjusting the content of PO43− anions added during the catalyst preparation process.
As shown in Table S3 (SM), the actual loadings of Ru metal on different Ru/TiO2 catalyst surfaces were concentrated between 0.92 wt% and 0.96 wt%, indicating that PO43− anions had no significant effect on the loading process of Ru metal. In addition, the surface areas of different Ru/TiO2 catalysts ranged from 68.40 m2/g to 69.16 m2/g, pore volume distributions ranged from 0.12 cm3/g to 0.21 cm3/g, and pore size distributions ranged from 7.17 nm to 7.82 nm. No significant abrupt changes were detected, indicating that the PO43− anions had no significant effect on the surface physicochemical properties of different Ru/TiO2 catalysts.
The structural characteristics of the catalyst were analyzed through XRD patterns. The XRD patterns of the different Ru/TiO2 catalysts are shown in FIG. 1. The diffraction peaks of the prepared Ru/TiO2 catalyst matched well with the standard card, and the diffraction peaks at 25.3°, 37.9°, 48.1°, 53.9°, and 55.1° correspond to (101), (004), (200), (105), and (211) crystal planes of anatase titanium dioxide (PDF# 87-0920) [26], respectively (FIG. 1(a)). In addition, no obvious diffraction peaks attributed to Ru metal nanoparticles were observed in FIG. 1(b), which may be attributed to the small size and low loading of Ru metal particles [27].
The surface electronic environments of the elements in the different Ru/TiO2 catalysts were explored through XPS. As shown in FIG. 2(a), the binding energy of the Ru species in the Ru/TiO2-0 catalyst synthesized without PO43− anion modification was 280.6 eV, corresponding to the 3d5/2 orbitals of the Ru0 species [28]. Compared with the binding energies of the Ru species of different Ru/TiO2 catalysts, the binding energy of the Ru species gradually decreased with increasing PO43− anion content, which indicated that the Ru species modified with PO43− anions had a relatively high surface electron cloud density. The Ru/TiO2-3 catalyst with the highest PO43− anion content had the lowest binding energy of the Ru species, and the binding energy was 280.0 eV. These results indicated that there may be strong interactions between PO43− anions and Ru species, therefore, the surface electron cloud density of Ru species could be regulated by PO43− anions. The binding energies of the Ti species in the different Ru/TiO2 catalysts are shown in FIG. 2(b). The binding energies at 458.5 and 464.2 eV belong to the 2p3/2 and 2p1/2 orbitals of the Ti4+ species of the TiO2 support [29], and there was no significant shift in binding energy positions before and after PO43− anion modification. Similar results were also obtained for the O species spectrum. As shown in FIG. 2(c), the binding energies at 529.7 and 531.5 eV correspond to the O 1s orbital of lattice oxygen species and surface hydroxyl oxygen species, respectively [30]. There was no significant shift in the binding energy positions of O species before and after PO43− anion modification. The above results reveal that after PO43− anion modification, the binding energies of the Ru species of the different Ru/TiO2 catalysts were significantly regulated, whereas there was no significant effect on Ti and O species, indicating that the modification of PO43− anions mainly act on Ru sites rather than on Ti and O sites. In addition, photoelectron peaks belonging to the PO43− species were clearly observed on the Ru/TiO2-3 catalyst surface (FIG. 2(d)). The photoelectron peaks located at 134.0 and 133.0 eV belong to the 2p1/2 and 2p3/2 orbitals, respectively, of the PO43− species [31], further demonstrating the successful modification of PO43− anions on the Ru/TiO2 catalyst surface.
The size and particle distribution of the Ru metal nanoparticles of different Ru/TiO2 catalysts were analyzed by TEM. As shown in FIG. 3(a), Ru metal nanoparticles were dispersed on the TiO2 support. In the HR-TEM image of the upper right corner, lattice stripes with an interplanar spacing of 0.214 nm, corresponding to the (002) crystal plane of metal Ru [32], were clearly observed, indicating the successful synthesis of the TiO2-supported Ru metal nanoparticle catalyst. Similarly, uniformly dispersed Ru metal nanoparticles and lattice stripes attributed to Ru metal were also observed on the surfaces of the Ru/TiO2-1, Ru/TiO2-2, and Ru/TiO2-3 catalysts (FIG. 3(b−d)). As shown in the lower right corner of FIG. 3, the average sizes of the Ru metal nanoparticles in the Ru/TiO2-0, Ru/TiO2-1, Ru/TiO2-2, and Ru/TiO2-3 catalysts were 1.18, 1.28, 1.27, and 1.33 nm, respectively. No significant difference in particle size was observed, indicating that PO43− anion modification has no significant effect on the particle size of Ru metal nanoparticles in the synthesized different Ru/TiO2 catalysts.
The above characterization results confirm the successful synthesis of Ru/TiO2 catalysts modified with PO43− anions. Moreover, the modification of PO43− anions has no significant effect on the physical or chemical properties, such as the crystal structure, surface area, or pore size, as well as the loading amount and size of Ru metal or the binding energy of Ti and O species. Instead, the PO43− anions regulate the surface electronic environment of Ru metal, indicating a strong interaction between the Ru metal and the modified PO43− anions on the catalyst surface.
-
To further investigate the interaction between PO43− anions and the Ru/TiO2 catalyst, the adsorption configuration of PO43− anions on the Ru, Ti, and O sites on the Ru/TiO2 catalyst surface was simulated through theoretical calculations. As shown in FIG. 4 (a) and (b), PO43− anions can stably adsorb on Ru and Ti sites, however, they cannot stably adsorb on O site. Calculations show that PO43− anions have the strongest adsorption energy (−6.65 eV) when they are adsorbed on Ru metal sites, followed by Ti sites (−3.51 eV) and O sites (−2.12 eV), indicating that the PO43− anions adsorbed on Ru sites are the most stable structure.
The differential density equipotential surfaces of PO43− anions adsorbed on Ru and Ti sites were subsequently further simulated to investigate the Ru site on the catalyst surface as the main action site of PO43− anion. As shown in FIG. 4(c), when PO43− anions were adsorbed on the Ru site, the number of electrons around the Ru metal and PO43− anions changes obviously, this finding reveals that significant electron transfer behaviour occurred between PO43− anions and Ru metal. However, when PO43− ions were adsorbed on Ti sites (FIG. 4(d)), a significant electron transfer process occurred. Therefore, PO43− anions, whether adsorbed on Ru or Ti sites, can also undergo a significant electron transfer process. However, on the basis of the XPS results, PO43− anions regulate the binding energy of Ru metal sites, whereas the binding energy of Ti does not significantly change, indicating that Ti site was not the adsorption site of PO43− anion. In addition, the adsorption configuration simulation of PO43− anions revealed that PO43− anions have a higher adsorption energy when they are adsorbed on Ru sites. Therefore, various characterization and theoretical calculation simulation results prove that the PO43− anions mainly adsorb on Ru metal sites on the modified Ru/TiO2 catalyst surface and that there is a strong interaction between PO43− anions and Ru sites, regulating the electronic environment of the Ru sites.
-
The catalytic performance of the PO43−-modified Ru/TiO2 catalysts was investigated by CO2 hydrogenation experiments. In the performance evaluation, we explored the effect of reaction solvents on catalyst performance. As shown in Table S4 (SM), when Ru/TiO2-3 was the catalyst, the CO2 conversions in water, DMF, and decalin were 7.2%, 11.6%, and 17.8%, respectively, and the hydrogenation product was mainly CH4. This finding indicates that the Ru/TiO2-3 catalyst has the best catalytic performance in decalin solvents. In addition, decalin has been developed as an effective hydrogen donor for hydrogenation reactions [33]; therefore, we chose decalin as the reaction solvent for the CO2 hydrogenation system. As shown in FIG. 5(a), when the reaction temperature was 300 °C, the catalytic activity of the Ru/TiO2-0 catalyst without PO43− anions was the worst with CO2 conversion of 3.6%, and CO was the main hydrogenation product with a selectivity of 98.2%, which indicated that the Ru/TiO2 catalyst without PO43− anion modification tended to synthesize CO products. Following the modification of different amounts of PO43− anions, the conversion of CO2 gradually increased, whereas the selectivity of CO decreased, and CH4 gradually became the main product. The Ru/TiO2-3 catalyst exhibited the highest hydrogenation performance of CO2, the conversion of CO2 increased by 4.9 times (17.8%), and the selectivity of CH4 was 97.5%. This indicates that PO43− anion modification was beneficial for obtaining CH4 products with high selectivity. In addition, the Ru/TiO2 catalysts modified with PO43− anions exhibited higher CO2 hydrogenation activity. The results of the XPS spectrum analysis revealed that the Ru metal nanoparticles modified with PO43− anions had a lower binding energy and were in an electron-rich state. This finding suggests that electron-enriched Ru metal is more likely to activate H2 and therefore exhibits higher catalytic activity. When the reaction temperature was 200 °C (FIG. 5(b)), the catalytic activity of the above catalyst significantly decreased, but no significant change was observed in the selectivity of the products, indicating that the change in temperature had no significant effect on the selectivity of the catalyst.
In addition, with the introduction of PO43− anions, Na+ ions were also introduced into the catalyst system; thus, further exploration of the role of Na+ ions is necessary. In accordance with a similar preparation process, we replaced the sodium phosphate added in the catalyst preparation process with sodium chloride or sodium nitrate and named the Ru/TiO2-Cl or Ru/TiO2-N catalyst, then explored its catalytic activity. As shown in FIG. S1 (SM), the products of CO2 hydrogenation catalysed by the Ru/TiO2-Cl and Ru/TiO2-N catalysts were still CO and resulted in poor CO2 conversion. The surfaces of the Ru/TiO2-Cl and Ru/TiO2-N catalysts also contain Na+ ions, but the introduction of Na+ ions does not affect the CO2 hydrogenation products, which shows that Na+ ions are not a factor affecting product selectivity in the Ru/TiO2 catalyst system modified by PO43− anions.
The modification of PO43− anions not only regulates the product selectivity of CO2 on the Ru/TiO2-3 catalyst surface but also increases the hydrogenation efficiency of CO2. Therefore, it is necessary to discuss whether the introduction of Na+ ions affects the hydrogenation efficiency of CO2. We used a pre-Ru/TiO2-3 catalyst without a high-temperature H2 reduction step for CO2 hydrogenation experiments. The surface Na+ and PO43− anion contents of the pre-Ru/TiO2-3 and Ru/TiO2-3 catalysts should be similar, but the Ru species in the pre-Ru/TiO2-3 catalyst were trivalent, whereas the Ru species in the Ru/TiO2-3 catalyst were zero valent. As shown in FIG. S2 (SM), compared with that of the Ru/TiO2-3 catalyst, the conversion of CO2 over the pre-Ru/TiO2-3 catalyst surface significantly decreased, but the product selectivity of the two catalysts was similar. This result was attributed to the greater ability of Ru metal to activate H2 than Ru3+ ions, resulting in higher CO2 hydrogenation efficiency. The above results indicate that the surface electronic environment of Ru species was the key factor affecting the efficiency of CO2 hydrogenation and that the surface of Ru sites enriched with electrons exhibited higher CO2 hydrogenation efficiency. In our designed Ru/TiO2 catalyst system, as the concentration of modified PO43− anions increases, the binding energy of Ru species gradually decreases. These results indicate that the modification of PO43− anions results in Ru metal with enriched surface electrons, increasing the ability to activate H2, which is beneficial for obtaining higher CO2 conversion efficiency. Therefore, the effect of Na+ ions on CO2 hydrogenation efficiency was excluded.
-
The hydrogenation process of CO2 on different Ru/TiO2 catalyst surfaces was analyzed by in situ diffuse reflectance infrared Fourier transform spectroscopy (in situ DRIFTS). As shown in FIG. 6(a), for the Ru/TiO2-3 catalyst, strong absorbance bands were observed at 1692, 1605 and 1313 cm−1, which were attributed to the characteristic absorbance bands of formate species [34, 35]. In addition, the absorbance band attributed to monodentate (m-CO32−, 1503 cm−1), multidentate carbonate (p-CO32−, 1411 cm−1),
$ {\rm HCO_3}^* $ species (1372 cm−1), and bicarbonate (b-CO32−, 1286 cm−1) also gradually increased [36−38]. The strong absorbance bands at 1749 and 3015 cm−1 were attributed to the characteristic absorbance bands of$^*{\rm CHO}$ and${{\rm CH}_x}^*$ species [39, 40]. The spectral information of these absorbance bands indicates that on the Ru/TiO2-3 catalyst surface, CO2 hydrogenation generates intermediates such as b-CO32−, p-CO32−, and${\rm HCO_3}^*$ , which undergo a methane reaction through the$ {\rm HCOO}^* $ pathway. Moreover, the CO intermediate generated on the catalyst surface undergoes further hydrogenation to produce$^*{\rm CHO}$ species, resulting in the final CH4 product. For the Ru/TiO2-0 catalyst (FIG. 6(b)), strong absorbance bands corresponding to$ {\rm HCOO}^* $ , b-CO32−, p-CO32−, m-CO32−, and$ {\rm HCO_3}^* $ were also observed, indicating that CO2 also underwent hydrogenation through the$ {\rm HCOO}^* $ pathway. However, no characteristic absorbance bands belonging to$^*{\rm CHO}$ or${{\rm CH}_x}^*$ species were observed in the spectrum. These results indicate that the CO intermediate generated on the Ru/TiO2-0 catalyst surface undergoes desorption rather than further hydrogenation, resulting in high selectivity for the CO product. On the basis of the information obtained from in situ DRIFTS, we speculate that the modification of PO43− anions may affect the adsorption and desorption properties of the Ru/TiO2 catalyst for CO intermediates in the CO2 hydrogenation process. The Ru/TiO2-3 catalyst strongly adsorbs CO intermediates, which results in further hydrogenation to obtain CH4 products. However, the adsorption strength of CO on the Ru/TiO2-0 catalyst surface was weaker, making it more prone to undergo desorption and obtain highly selective CO products.CO-TPD was subsequently used to investigate the adsorption characteristics of CO intermediates on different Ru/TiO2 catalysts surfaces to investigate the reasons for the transformation of CO2 hydrogenation products before and after PO43− anion modification. As shown in FIG. 7(a), the characteristic peak at 213 °C was attributed to the linear adsorption of CO on the Ru metal sites [41], whereas the characteristic peaks at 334 and 564 °C were attributed to the bridge adsorption of CO at the Ru metal sites [42]. With respect to the Ru/TiO2-0 catalyst, a weak CO adsorption peak could be observed, indicating weak adsorption of CO by the Ru/TiO2-0 catalyst. With respect to the Ru/TiO2-3 catalyst, the intensity of the CO adsorption peak significantly increased, indicating that the Ru/TiO2-3 catalyst has better CO adsorption characteristics.
In addition, DRIFTS characterization was also used to investigate the adsorption characteristics of CO on different Ru/TiO2 catalyst surfaces. As shown in FIG. 7(b), the absorbance band at 1988 cm−1 corresponds to the bridge adsorption of CO at the Ru0 sites [43, 44]. The absorbance band at 2059 cm−1 was attributed to the linear adsorption of CO on the Ru0 sites [45]. A strong CO absorbance band was observed on the Ru/TiO2-3 catalyst surface, which was beneficial for further hydrogenation to obtain the CH4 product. However, for the Ru/TiO2-0 catalyst, the absorbance band intensity of CO was significantly weakened, which was not conducive to the continued hydrogenation of CO and resulted in CO becoming the main product. The results of CO-TPD and DRIFTS confirmed our hypothesis. The modified PO43− anions act on the Ru metal sites of the Ru/TiO2-3 catalyst, affecting the adsorption and desorption properties of Ru metal towards CO intermediates and thereby regulating the selectivity of CO2 hydrogenation products.
Further investigations are needed to determine the structural and performance stability of the catalyst, and we investigated the stability of the Ru/TiO2-3 catalyst. As shown in FIG. S3 (SM), the conversion and selectivity of the Ru/TiO2-3 catalyst did not show significant differences during 5 cycles of CO2 hydrogenation, indicating good performance stability. The structural stability of the Ru/TiO2-3 catalyst after cycling was subsequently investigated through XRD, XPS, and TEM characterization. As shown in FIG. S4 (SM), no significant differences in diffraction peaks were observed in the XRD patterns of the Ru/TiO2-3 catalyst after 5 cycles. In the XPS spectrum (FIG. S5 in SM), there was no significant shift in the binding energy of Ru metal in the cycled Ru/TiO2-3 catalyst. In the TEM images (FIG. S6 in SM), the Ru nanoparticles were still uniformly dispersed on the TiO2 support surface, and no obvious particle aggregation was detected. The above results indicate that the Ru/TiO2-3 catalyst modified with PO43− anions has excellent catalytic performance stability and structural stability.
-
In conclusion, we innovatively reported that the complete conversion of CO2 hydrogenation products from CO to CH4 could be achieved over a Ru/TiO2 catalyst surface by modification with PO43− anions. The Ru/TiO2-0 catalyst without PO43− anion modification shows poor CO2 hydrogenation activity, and the main product obtained is CO, whereas the Ru/TiO2-3 catalyst modified by PO43− anions shows high conversion of CO2 and is more inclined to produce CH4. XPS and theoretical calculation simulation results reveal that the PO43− anions mainly act on the Ru metal site on the Ru/TiO2 catalyst surface, which regulates the surface electronic properties of Ru metal and affects its catalytic performance for CO2 conversion. In addition, the results of CO-TPD and DRIFTS reveal that the adsorption characteristics of CO intermediates are improved by Ru sites after PO43− anion modification; thus, highly selective CH4 products were obtained. The results of the cycling experiments and characterization confirm that the Ru/TiO2 catalyst modified by PO43− anions exhibits excellent performance and structural stability. Our research explore in depth the regulation of the characteristics of metal-based catalysts by anion modification, providing valuable guidance for the synthesis of catalysts with specific catalytic performance.
Supplementary materials: Additional catalyst characterization, and supplementary experiments, including ICP-OES, ion chromatography, BET surface area, pore volume, pore area, catalyst cycle test experiment, XRD patterns, XPS spectra, TEM and HR-TEM images.
-
The authors have no conflict of interest to declare.
Ru/TiO2 Catalyst Modified by Phosphate Anion: Realizing Specific Transformation of CO2 Hydrogenation Products
- Received Date: 07/09/2025
- Available Online: 27/08/2026
-
Key words:
- CO2 hydrogenation /
- Anion modification /
- Selectivity regulation /
- Ru/TiO2 /
- CH4/CO
Abstract: Regulation of the CO2 hydrogenation process to obtain highly selective target products is a challenging and important research topic. In this study, we report the key role of PO43− anions modified on the Ru/TiO2 catalyst surface in regulating the CO2 hydrogenation process. Ion chromatography, X-ray diffraction, X-ray photoelectron spectroscopy, and transmission electron microscopy confirmed the successful preparation of the Ru/TiO2 catalyst modified by PO43− anions. The original Ru/TiO2 catalyst showed poor catalytic activity in CO2 hydrogenation, and the main hydrogenation product was CO. With the PO43− anion-modified Ru/TiO2 catalysts, the conversion of CO2 was clearly improved, and the hydrogenation product changed from CO to CH4. XPS characterization and DFT theoretical calculations confirmed that the modified PO43− anions interacted mainly with the Ru metal site on the Ru/TiO2 catalyst surface, effectively regulating the surface electronic properties of the Ru metal, which affected the conversion efficiency of CO2. In addition, CO temperature-programmed desorption and diffuse reflectance infrared Fourier transform spectroscopy characterization revealed that the adsorption of CO intermediates improved after the Ru metal surface was modified with PO43− anions, which was beneficial for further CO hydrogenation and the formation of CH4 products. Our work expands the research strategies of anion-modified metal-based catalysts that regulate the hydrogenation performance of CO2 and provides a new direction for further understanding the influence mechanism of the catalyst surface structure on hydrogenation performance.