2025 Volume 34 Issue 10
Article Contents

Zijie Zhou, Junning Zhao, Xinhui Ma, Rong Wang, Fusheng Ma. Coupling of magnon modes in nanodisk with spin texture[J]. Chinese Physics B, 2025, 34(10): 107506. doi: 10.1088/1674-1056/ade426
Citation: Zijie Zhou, Junning Zhao, Xinhui Ma, Rong Wang, Fusheng Ma. Coupling of magnon modes in nanodisk with spin texture[J]. Chinese Physics B, 2025, 34(10): 107506. doi: 10.1088/1674-1056/ade426

Coupling of magnon modes in nanodisk with spin texture

  • Received Date: 31/03/2025
    Accepted Date: 12/06/2025
    Available Online: 01/10/2025
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

Figures(4)

Article Metrics

Article views(442) PDF downloads(1) Cited by(0)

Access History

Coupling of magnon modes in nanodisk with spin texture

Abstract: Magnetic nanostructures with nonhomogeneous magnetic properties exhibit distinct magnon modes, and their interactions are crucial for understanding magnetization dynamics. In this work, we numerically investigate the magnon–magnon coupling in a nanodisk with radially varying magnetic anisotropy by using micromagnetic simulations. By introducing perpendicular magnetic anisotropy into the inner region of the nanodisk, a radially chiral spin texture is observed. The presence of the chiral spin texture results in coupling between the ferromagnetic resonance mode of the whole disk and the higher-order confined modes in the outer region. Moreover, we find that the coupling strength is highly sensitive to the perpendicular magnetic anisotropy, the saturation magnetization, and the interfacial Dzyaloshinskii–Moriya interaction. Our findings could enrich the understanding of the dynamic characteristics of chiral nanomagnets and suggest a possible route to harnessing tunable magnon–magnon coupling for spin-based quantum information processing.

1.   Introduction
  • Magnetic chirality refers to the handedness of spin arrangements, a characteristic commonly found in certain spin-ordered states or nanoscale spin textures.[1–5] The Dzyaloshinskii–Moriya interaction (DMI) is recognized as a fundamental interaction that induces the formation of chiral spin structures such as magnetic skyrmions.[6,7] In magnetic thin films, the interfacial DMI is the principal mechanism that gives rise to distinctive chiral spin textures, i.e., chiral domain walls,[8] spin spirals,[9] radial vortices,[10–12] and skyrmions.[13,14] Chiral spin textures hold great promise for realizing information storage and processing functions, such as racetrack memory,[15] logic devices,[16] transistors, oscillators,[13] and frequency combs,[16] thereby significantly facilitating the development of novel spintronic devices.

    Cavity magnonics has attracted great attention due to its potential applications in coherent information processing.[17–20] As quanta of spin waves, magnons possess short wavelengths, high frequencies (up to the terahertz regime), non-Ohmic dissipation, and easy tunability.[21–23] These advantages open the possibility of developing energy-efficient magnonic devices for quantum information operations.[24,25] The coupling between magnons and other quasiparticles or excitations has been studied in a variety of systems, such as magnon–photon,[26–28] magnon–magnon,[29,30] magnon–phonon,[31–33] and magnon–superconducting-qubit interactions.[34–36] Among them, magnon–magnon coupling has been investigated toward the miniaturization and integration of spintronic devices.[37–40] The coupling between the ferromagnetic resonance (FMR) mode and the standing spin-wave (SSW) mode has been reported in Ni/YIG and Co/YIG heterostructures, respectively.[28,30] Recent studies have demonstrated that the coupling between the optical mode and the acoustic mode in synthetic antiferromagnets can reach the strong, ultra-strong, and deep-strong regimes.[41–43] The magnon–magnon coupling within an individual magnetic single layer has also been realized in, for instance, an irregular hexagonal dot and a cross-shaped nanoring.[44–48] Very recently, it has been found that magnetic nanostructures with nonhomogeneous material properties can exhibit diverse spin configurations in the presence of interfacial DMI.[2] The coupling between magnon modes confined in such nonhomogeneous magnetic nanostructures is therefore worth exploring.

    In this work, we perform micromagnetic simulations to numerically investigate the coupling between magnons in a magnetic nanodisk with radially varying magnetic anisotropy. The chiral spin texture is obtained by introducing the interfacial DMI and the radially distributed perpendicular magnetic anisotropy (PMA). We find that the FMR mode of the entire nanodisk can couple with various radial modes confined in the outer ring-shaped (OR) region. The tunability of the coupling is verified by varying the PMA, saturation magnetization, and interfacial DMI. Our findings demonstrate that chiral nanomagnets could serve as an excellent platform for exploring coupling phenomena within the field of cavity magnonics.

2.   Model and simulation method
  • Figure 1(a) schematically shows the magnetic nanodisk used, with a spatially distributed magnetic anisotropy along the radial direction, i.e., the inner circular (IC) region possesses PMA. The diameters of the nanodisk and the IC region are represented by d1 and d2, respectively. The micromagnetic simulations are performed using Mumax3.[49] During the simulations, the nanodisk is discretized into cubic cells with a size of 1 nm × 1 nm × 1 nm along the x, y, and z axes, respectively. The material parameters used in the simulations are adopted from the Pt/Co/Al system: saturation magnetization Ms = 9 × 105 A/m, exchange stiffness constant A = 1.6 × 10−11 J/m, interfacial DMI constant D = 1.5 × 10−3 J/m2, damping constant α = 0.01, and PMA constant Ku = 5.7 × 105 J/m3.[2,47]

    The magnetization distribution and magnon modes under different bias fields Hz are calculated through a two-step simulation procedure. Firstly, the magnetization distribution is obtained by minimizing the total energy of the system under each Hz. Secondly, to excite magnons with frequencies ranging from 0 GHz to 100 GHz, a spatially uniform sinc-function-type perturbation field of the form hrf(t) = h0sin(2πfct)/(2πfct) is applied along the x-axis, where the amplitude is h0 = 5 mT and the cut-off frequency is fc = 100 GHz.[50] Alternatively, to excite magnons at a fixed frequency f and to obtain the corresponding mode profiles, a sinusoidal perturbation field hx(t) = h0sin(2πft) is applied along the x-axis. For the dynamic simulations under each Hz, the temporal evolution of the spatially averaged magnetization m(t) is recorded, with a time step of Δt = 10 ps. The magnon spectra are obtained by performing a fast Fourier transform (FFT) on the spatially averaged mx(t). The mode profiles of magnons are characterized by temporal snapshots of the magnetization variation, defined as Δmx(t) = mx(t) – mx(0).

3.   Results and discussion
  • The investigated nanodisk consists of two regions: the IC region with perpendicular magnetic anisotropy Ku = 5.7 × 105 J/m3 along the z-axis, and the OR region with zero Ku, as schematically illustrated in Fig. 1(a). The calculated magnetization–field (mz–Hz) loops of the nanodisk are shown in Fig. 1(b) for d2 = 100 nm and d1 = 135 nm, 170 nm, and 205 nm. The slope of the magnetization curve increases with larger d1. The insets in Fig. 1(b) display the magnetization distributions for d1 = 170 nm at Hz = 200 mT, 500 mT, and 800 mT, respectively. The observed chiral spin textures arise from the competition among DMI, exchange interaction, and magnetic anisotropy.

    We first focus on the nanodisk with d1 = 170 nm, as shown in Figs. 1(c) and 1(d). The magnon spectra of the IC and OR regions are separately calculated, and the corresponding frequency–field (f–Hz) dispersions are presented in Figs. 1(c) and 1(d). Figure 1(d) shows the f–Hz dispersion of the OR region alone, with the magnetization of the IC region fixed. The fixed out-of-plane magnetization in the IC region still exerts a significant static influence on the magnon modes confined within the OR region. This interaction disturbs the spatial uniformity required for coherent precession, thereby suppressing the visibility of the FMR mode in the OR region.

    For the IC region, two distinct magnon modes, labeled (i) and (ii), are identified in Fig. 1(c). The inset shows the corresponding spectrum at Hz = 200 mT. Based on the spatial mode profiles in Fig. 1(e), mode (i) is recognized as the first radial mode (the ferromagnetic resonance, or FMR mode), characterized by a nearly uniform precession without radial nodes. Mode (ii) is identified as the second radial mode, exhibiting a single radial node in the magnetization distribution.

    In contrast, for the unsaturated OR region, three distinct magnon modes, (iii), (iv), and (v), are observed, as indicated in Fig. 1(c). These modes exhibit combined azimuthal and radial characteristics and can be indexed by (radial, azimuthal) numbers. They correspond to the spatially confined (0, +2), (0, −2), and (1, +2) modes, respectively, as shown in Fig. 1(e). For clarity, the color maps of all mode profiles in Fig. 1(e) are individually normalized to their maximum Δmx amplitude. Modes (iii) and (iv) are low-frequency gyrotropic modes, with the signs +/− denoting counterclockwise/clockwise propagation directions. Mode (v), having a higher frequency than (iii) and (iv), exhibits counterclockwise propagation and features one azimuthal and two radial nodes. Although some modes share the same azimuthal number m, differences in their radial node numbers lead to distinct spatial distributions.

    Next, Fig. 2(a) presents the f–Hz color plot of the nanodisk with d1 = 170 nm and d2 = 100 nm. The high- and low-frequency branches clearly exhibit coupling features, such as the characteristic “anti-crossing” behavior and pronounced intensity exchange. The coupling parameters are analyzed as follows: the coupling strength g = |f1 – f2|/2, the coupling magnetic field Hg, and the coupling center frequency fg = |f1 + f2|/2, where f1 and f2 are the frequencies of the upper and lower magnon modes at Hg.

    To identify which magnon modes participate in the coupling, we extract the mode frequencies in the IC region, OR region, and the whole nanodisk, as shown in Fig. 2(b). Figure 2(c) shows the radial intensity distributions of the FMR mode, the (1, +2) mode, and the coupling mode (CM) for Hz = 320 mT. The temporal variation of magnetization Δmx(x,t) along the radius is normalized to indicate the relative magnon intensity.[50] The intensity distributions reflect the overall dynamic response of the coupled state. It can be seen that the (1, +2) mode strongly influences the precession near the IC–OR interface, while the FMR mode extends across the entire nanodisk. The CM exhibits a hybridized character that combines features of both.

    To further verify the mode origins, Fig. 2(d) displays normalized Δmx intensity maps of modes I–IV (labeled in Fig. 2(b)). Each color map is normalized to its own maximum value. At Hz = 320 mT (near Hg), the profiles of modes I and II indicate strong hybridization between the FMR and (1, +2) modes. At Hz = 600 mT (far from Hg), the hybridization largely vanishes, as shown by modes III and IV. Furthermore, Fig. 2(e) presents the radial intensity distributions of modes I–IV at t = 0 and T/2, marked by the dashed lines in Fig. 2(d). The results show that mode III corresponds to the (1, +2) mode, mode IV to the FMR mode, and mode II to the coupled mode, which is a superposition of both.

    Compared with the FMR mode, the (1, +2) mode exhibits a weaker magnetic-field dependence, allowing the two magnon modes to intersect and couple. Higher-order radial magnon modes have a similar f–Hz slope to that of the first radial mode, implying that coupling with the FMR mode is also possible.

    According to the characteristics of radial magnons, higher-order radial modes can be excited by increasing the diameter of the OR region. As an example, Fig. 3(a) shows the color plots of the f–Hz dispersion obtained for d1 = 190 nm and d2 = 100 nm. The intensity distributions of Δmx along the radius for various magnon modes b, c, d, and e are shown in Figs. 3(b)–3(e), respectively, as labeled by triangles in Fig. 3(a). It is clearly observed that modes c and e are FMR modes, while modes b and d are confined modes in the OR region with different node configurations, (1, +2) and (2, +2). In Fig. 3(a), the lower anti-crossing arises from the coupling between the FMR mode and the (1, +2) mode, whereas the higher anti-crossing results from the coupling between the FMR mode and the (2, +2) mode. Therefore, it is expected that the coupling between the FMR mode and even higher-order radial magnon modes can be achieved by further increasing d1.

    To investigate the influence of magnetic parameters on the coupling, we study the nanodisk by varying D, Ku, and Ms, respectively.

    First, Fig. 4(c) illustrates the effect of Ms in the range from 8.1 × 105 A/m to 9.9 × 105 A/m. It is observed that g and fg decrease from 2.39 GHz to 1.63 GHz and from 14.84 GHz to 13.68 GHz, while Hg increases from 41 mT to 470 mT. The increasing Ms enhances the demagnetizing field, which flattens the magnetization at the boundary between the IC and OR regions, i.e., broadens the transition region.[51] This reduced spatial overlap between the magnon modes suppresses the coupling strength.[52]

    Second, the effect of Ku in the IC region is examined within the range from 5.1 × 105 J/m3 to 6.3 × 105 J/m3, as shown in Fig. 4(b). Hg, g, and fg exhibit distinct dependences on Ku: g increases from 1.79 GHz to 2.06 GHz, Hg decreases from 410 mT to 150 mT, and fg remains nearly constant around 14.50 GHz. The increasing Ku enhances the out-of-plane alignment of magnetization in the IC region, causing the transition region at the IC–OR boundary to become narrower.[53] This leads to increased spatial overlap between the magnon modes, thereby enhancing the coupling strength. Moreover, a higher Ku strengthens the internal effective field and raises the intrinsic resonance frequency of the IC region, shifting the mode crossing point to a lower external field.

    Third, the dependence of Hg, g, and fg on D is shown in Fig. 4(a). With D increasing from 1.5 to 2.5 × 10−3 J/m2, g decreases from 1.90 GHz to 1.66 GHz, fg increases from 14.55 GHz to 16.38 GHz, and Hg increases from 280 mT to 340 mT. With increasing D, the DMI favors non-collinear alignment between the magnetizations in the IC and OR regions, thereby enlarging the angular deviation and broadening the magnetization transition region. This reduces the spatial overlap between the FMR and (1, +2) modes, thus weakening the coupling strength.[54] A stronger external field H is required to overcome this non-collinear tendency, leading to an increase in Hg. Since the coupling occurs within a single-layer nanodisk, it is primarily mediated by exchange interaction, which dominates when the interacting spin-wave modes exhibit strong spatial overlap, while the dipolar interaction plays a negligible role in such confined geometries.[55–57]

4.   Conclusion
  • In summary, we numerically study the magnon–magnon coupling in a magnetic nanodisk with a radially chiral spin texture, which is realized through the introduction of interfacial DMI and radially distributed PMA. The observed coupling is attributed to the interaction between the FMR mode of the entire nanodisk and the higher-order confined modes in its outer ring-shaped region. It is also found that the coupling phenomena are highly sensitive to D, Ku, and Ms. The coupling strength increases with Ku but decreases with D and Ms. This work provides new insights into the dynamic characteristics of chiral nanomagnets, highlighting them as a promising platform for exploring magnon coupling phenomena.

Figure (4)  Reference (57)

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint