2026 Volume 35 Issue 8
Article Contents

Zhun Li, Xinrun Mi, Xinmin Wang, Jian Lyu, Na Su, Aifeng Wang, Yisheng Chai, Bao Yuan, Wanju Luo, Hui Cheng, Jianxiang Gao, Hongliang Wang, Lijie Hao, Mingquan He, Junying Shen, Young Sun, Xin Tong. Pressure tunable magnetic skyrmion phase in Co8Zn8Mn4 single crystals[J]. Chinese Physics B, 2026, 35(8): 086103. doi: 10.1088/1674-1056/ae13ed
Citation: Zhun Li, Xinrun Mi, Xinmin Wang, Jian Lyu, Na Su, Aifeng Wang, Yisheng Chai, Bao Yuan, Wanju Luo, Hui Cheng, Jianxiang Gao, Hongliang Wang, Lijie Hao, Mingquan He, Junying Shen, Young Sun, Xin Tong. Pressure tunable magnetic skyrmion phase in Co8Zn8Mn4 single crystals[J]. Chinese Physics B, 2026, 35(8): 086103. doi: 10.1088/1674-1056/ae13ed

Pressure tunable magnetic skyrmion phase in Co8Zn8Mn4 single crystals

  • Received Date: 01/08/2025
    Accepted Date: 10/10/2025
    Available Online: 01/08/2026
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

Figures(4)  /  Tables(1)

Article Metrics

Article views(81) PDF downloads(0) Cited by(0)

Access History

Pressure tunable magnetic skyrmion phase in Co8Zn8Mn4 single crystals

Abstract: In a magnetic skyrmion phase, magnetic moments form vortex-like topological textures which are of both fundamental and industrial interest. In β-Mn-type Co–Zn–Mn alloys, chiral magnetic skyrmions emerge above room temperature, providing a unique system for studying the skyrmion physics and exploring spintronics applications. However, the magnetic skyrmion phase is typically confined in a narrow and limited temperature (T) and magnetic field (H) range. Here, we demonstrate that quasihydrostatic pressure can expand the skyrmion phase in the T–H phase diagram of single-crystalline Co8Zn8Mn4. At ambient pressure, signatures of skyrmions are seen within T ∼ 302 K–308 K and H ∼ 50 Oe–100 Oe (1 Oe = 79.5775 A⋅m−1). Applying a moderate pressure of 6 kbar (1 bar = 105 Pa) extends this range to T ∼ 300 K–310 K and H ∼ 50 Oe–150 Oe. However, further escalation of pressure to 10 kbar results in a slight contraction of the skyrmion phase. These findings underscore the sensitivity of the skyrmion phase in Co8Zn8Mn4 to external pressures, and hint at the potential of strain engineering, particularly in β-Mn-type Co–Zn–Mn thin films, as a promising avenue to customize the skyrmion phase.

1.   Introduction
  • Magnetic skyrmions, distinguished by their unique vortex-like spin configurations carrying integer topological charges, have become a forefront in the study of condensed matter physics and material science.[1–3] The nontrivial spin textures of skyrmions are fascinating both from a fundamental physics perspective and for their potential technological applications. Fundamentally, magnetic skyrmions can arise through diverse mechanisms, such as the interplay between ferromagnetic exchange, Dzyaloshinskii–Moriya (DM), Ruderman–Kittel–Kasuya–Yosida (RKKY), and magnetic dipolar interactions.[2–7] From a technological standpoint, skyrmions stand out for their emergent electromagnetic properties and the ability to be manipulated with low current densities, making them highly efficient for advanced spintronics applications.[8–10]

    In bulk materials, magnetic skyrmions are commonly observed in chiral magnets, such as metallic B20 compounds (MnSi, Fe1−xCoxSi, FeGe) and insulating Cu2OSeO3.[2,3,11,12] In these non-centrosymmetric compounds, a helimagnetic state is typically formed below a certain magnetic Curie temperature (Tc) due to the competition between DM and ferromagnetic exchange interactions. In the presence of magnetic fields, a skyrmion crystal (SkX) phase emerges in the vicinity of Tc. However, the Tc values of the aforementioned chiral magnets lie below room temperature, limiting the applications of skyrmions. Interestingly, this limitation is overcome in another type of chiral magnets, i.e., the β-Mn-type CoxZnyMnz (x + y + z = 20) alloys.[13] The Curie temperatures of CoxZnyMnz depend strongly on compositions and Tc > 300 K can be realized when z ≤ 4.[13] Above room temperature, skyrmion lattices have been observed in a series of CoxZnyMnz.[13–18] Like the B20 compounds, the SkX phase in CoxZnyMnz is typically confined in a narrow temperature (T) and magnetic field (H) region near Tc, as a result of the interplay between long-range magnetic interactions and thermal fluctuations.[13–18] A goal in the study of skyrmions in bulk chiral magnets is to expand the temperature and magnetic field window which supports the SkX phase.

    It has been found that long-lived metastable skyrmions in CoxZnyMnz can survive in a wide temperature range well below Tc, achieved via the assistance of magnetic frustrations, disorders, or field-trained cooling.[14,18–20] In addition, pressure or strain is another effective tuning parameter in manipulating crystal structure, magnetic interactions, and magnetic phases. It has been theoretically suggested that uniaxial anisotropy induced by uniaxial strain can stabilize the skyrmion phase of MnSi, FeGe, and Fe1−xCoxSi in a broad temperature and magnetic field range.[21] Indeed, as found experimentally, the skyrmion phase in MnSi can be easily controlled by quasihydrostatic pressure,[22] uniaxial pressure,[23] and uniaxial stress.[24] Applying a moderate strain[25] or quasihydrostatic pressure[26] to Cu2OSeO3 significantly enlarges the skyrmion pocket spanned in the T–H phase diagram. Pressure control of the skyrmion phase in CoxZnyMnz alloys is, however, yet to be investigated.

    In this article, we study the effects of quasihydrostatic pressure on the skyrmion phase in single crystals of Co8Zn8Mn4. At ambient pressure, the skyrmion phase is found to exist within about 5 K just below Tc. This temperature window is almost doubled under a moderate pressure of 6 kbar. The magnetic field range of the skyrmion pocket is also enlarged under pressure. Pressure is thus a sensitive tuning knob in controlling the skyrmion phase in Co8Zn8Mn4.

2.   Experimental methods
  • Single crystals of Co8Zn8Mn4 were grown using the Bridgman method.[27] A precursor CoxZnyMnz (x + y + z = 20) was first synthesized via a solid-state reaction. Pure Co (99.99%), Zn (99.99%), and Mn (99.99%) grains were mixed in a quartz tube, which was then sealed in a vacuum environment. The mixture was heated to 1000 °C and kept at this temperature for 24 h. It was then slowly cooled down to 925 °C at a rate of 1 °C/h, followed by water quenching. Then the product was ground thoroughly in an agate mortar, and the precursor complexes of Co8Zn8Mn4 were obtained. Finally, we used these precursor complexes according to the method described in Ref. [28] to grow single crystals of Co8Zn8Mn4.

    The composition of the as-prepared single crystals was determined by energy-dispersive x-ray spectroscopy (EDX). Both powder x-ray diffraction and single-crystal x-ray diffraction (XRD) measurements were performed on a Malvern Panalytical EMPYREAN SERIES 3 diffractometer, and the latter was carried out on a large piece of Co8Zn8Mn4 single crystal (4.20 mm × 2.5 mm × 0.25 mm). Single-crystal neutron diffraction experiments were carried out on a four-circle neutron diffractometer in the Chinese Advanced Research Reactor. An incident beam with a wavelength of 0.9085 Å was used, selected by a vertically focusing Cu (220) monochromator crystal.

    DC magnetization and ac magnetic susceptibility of Co8Zn8Mn4 samples were measured in a superconducting quantum interference device magnetometer (MPMS-3, Quantum Design). For the ac magnetic susceptibility experiments, an excitation amplitude of 1 Oe and a frequency of 10 Hz were used. DC magnetization under pressure was measured in the magnetic properties measurement system (MPMS-3, Quantum Design) using a miniature piston pressure cell with Daphne 7373 as the pressure transmitting medium, and Sn was loaded into a Teflon capsule along with the sample. The applied pressure at low temperatures was determined by monitoring the pressure-dependent superconducting transition temperature of Sn. The corresponding pressure at room temperature was estimated by adding a constant of 1.6 kbar to the pressure obtained at low temperatures, as the pressure difference for the pressure-transmitting medium Daphne 7373 between 300 K and 4.2 K is consistently between 1.5 kbar and 1.7 kbar.[29] We note that although Daphne 7373 remains liquid up to about 30 kbar at room temperature,[30] pressure inhomogeneity inevitably exists (approximately 5% at 13.4 kbar and 300 K).[31] Therefore, only quasihydrostatic conditions were achieved in the temperature and pressure ranges studied here. For all field-dependent measurements, the external magnetic field was consistently applied along the [110] crystalline direction on the same crystal, with the field swept upwards.

    The magnetostriction coefficient of a Co8Zn8Mn4 single crystal was measured using a composite magnetoelectric (ME) method.[32,33] The Co8Zn8Mn4 sample was mechanically bonded to a piezoelectric PMN-PT [0.7Pb(Mg1/3Nb2/3)O3–0.3PbTiO3] transducer using silver epoxy. The PMN-PT is a [001]-cut thin plate with a thickness of 0.2 mm. In a magnetic field, the magnetostrictive length deformation of Co8Zn8Mn4 is transferred to PMN-PT, generating an electronic voltage via the piezoelectric effect. The recorded ME voltage coefficient αME can be formulated as

    where 0 < k < 1 is a strain transmission constant between the mechanically bonded Co8Zn8Mn4 sample and PMN-PT, λ is the magnetostriction, dλ/dH is the magnetostriction coefficient, and dE/dλ is the piezoelectric coefficient. During the experiments, a small ac magnetic field was superimposed on a DC magnetic field, giving rise to an ac ME signal αME = αx + iαy [see Fig. 3]. The ac magnetic field was generated by a homemade Helmholtz coil. An excitation amplitude of 1 Oe and a frequency of 422 Hz were used for the ac magnetostriction measurements. The ac ME data were collected using the lock-in technique.

3.   Results and discussion
  • β-Mn-type CoxZnyMnz (x + y + z = 20) alloys crystallize in a cubic structure belonging to the chiral space group P4132 [see Fig. 1(b) inset] or P4332.[27,34] These two types of space group host different chiralities and can be interchanged by a mirror operation. There are two different Wyckoff sites (8c and 12d) occupied by 20 atoms in each unit cell. The Co atoms are coordinated at the 8c sites, and the Zn/Mn atoms are located at the 12d sites.[13–18,35] Figure 1(a) shows the x-ray diffraction data obtained on Co8Zn8Mn4 powders. The observed data can be well described by the β-Mn cubic chiral structure. The refined lattice constants give a = b = c = 6.3617 Å, agreeing well with previous reports.[19] Detailed structure parameters are listed in Table 1. It is seen that minor Mn atoms also enter the 8c sites, which typically happens in CoxZnyMnz compounds with z ≥ 4.[16] In Fig. 1(b), x-ray diffraction patterns captured from a typical Co8Zn8Mn4 single crystal are shown. Two sharp peaks can be nicely indexed by (2,2,1) and (4,4,2), respectively. The quality of the Co8Zn8Mn4 sample is further checked by single-crystal neutron diffraction, as displayed in Figs. 1(c)–1(f). Rocking curves near four typical Bragg peaks are nicely resolved and both peaks show a very narrow full width at half maximum (FWHM) about 0.16 degrees, in good agreement with the reported data.[19] All these results point to the high quality of the single crystal.

    Figure 2 shows DC magnetization data of a Co8Zn8Mn4 single crystal. In a weak magnetic field (H = 20 Oe), a clear ferromagnetic-like transition is seen at Tc = 309 K in the temperature-dependent magnetization experiments [Fig. 2(a)]. The transition temperature is slightly higher than that (Tc∼300 K) reported in other studies.[13,18,19] This minor difference is likely caused by slight variations in compositions, since Tc is sensitive to the Mn concentration.[13,14,16,18] In zero field and below Tc, Co8Zn8Mn4 enters a helical magnetic state with a periodicity of λ ∼ 125 nm.[13,19] Below Tc, the temperature dependence of magnetization deviates from a typical ferromagnet, especially at low temperatures. Below about 150 K, the magnetization decreases gradually with cooling, both in zero-field-cooled (ZFC) and field-cooled (FC) measurements. In addition, a sharp drop is seen in ZFC data below Tg ∼ 20 K. The transition occurring at Tg is caused by a re-entrant spin-glass transition, which is commonly observed in CoxZnyMnz for 3 ≤ z ≤ 19.[14,16,18] It has been suggested that Co moments order magnetically below Tc, while Mn moments remain fluctuating with cooling until Tg, below which a spin-glass state is formed.[16,17] In Fig. 2(b), the magnetization near Tc is plotted as a function of magnetic field (H ∥ [110]). Below Tc, the magnetization rises rapidly with increasing magnetic field and becomes saturated above about 150 Oe. In the saturated region, magnetic moments are ferromagnetically polarized though the magnetization further increases slightly in higher fields. Slightly above Tc, nonlinear M(H) curves are also seen, suggesting sizable spin fluctuations. As shown in Fig. 2(a), the onset of the spin–spin correlation starts already below 330 K. And linear M(H) is almost restored at 320 K [Fig. 2(b)]. Note that signatures of skyrmions are masked by the rapid variations of magnetization in small magnetic fields. Transitions between different magnetic phases are seen more clearly in the derivative form dM/dH, as shown later in Fig. 4.

    To access the skyrmion phase, we present ac susceptibility χ = χ′ + iχ″ in Figs. 2(c) and 2(d). Between 302 K and 306 K, a clear dip is seen around 50 Oe in both the real (χ′) and imaginary (χ″) parts of ac susceptibility. This dip structure, commonly observed in skyrmion hosts B20 compounds and Cu2OSeO3,[12,36,37] is a characteristic thermodynamic signature of skyrmion lattice in Co8Zn8Mn4.[13] The magnetic fields H1 and H2 mark the lower and upper boundaries of the skyrmion pocket. As found by earlier reports, the skyrmion phase is sandwiched by conical states.[13,14,16,18] The H1 and H2 are thus critical fields differentiating the skyrmion and conical phases. The transition between the zero-field helimagnetic and conical states happens at a lower field H0, below which χ′ depends weakly on H. In the vicinity of a higher magnetic field H3, χ′ drops rapidly and a polarized ferromagnetic state is achieved above H3.

    In addition to the ac magnetic susceptibility, the ac ME coefficient, which is proportional to magnetostriction, is another thermodynamic probe for sensing the skyrmion phase.[32,33,38,39] Distinct magnetostrictive features have been observed in the skyrmion phase of MnSi[32,39] and Co7Zn8Mn5.[33] Figures 3(a) and 3(b) show the ac ME coefficient results of Co8Zn8Mn4. At temperatures above Tc, both the real (αx) and imaginary (αy) components of the ac ME coefficient vary smoothly with magnetic field. At 308 K, just below Tc, a kink in αx and a peak in αy are observed at H0, indicating the transition from the helical to conical phase. At a slightly higher magnetic field H1, a broad maximum in αx and a clear dip in αy mark the transition between the conical and skyrmion phases. Upon further cooling, these features at H0 and H1 become more pronounced [see Fig. 3(d)]. Near H2, αx rises steeply while αy becomes nearly field-independent, indicating the transition from the conical to ferromagnetic state, visualized as a broad peak in αx near H3. Below 302 K, signatures of the skyrmion phase gradually fade, consistent with the ac susceptibility data. In Figs. 3(c) and 3(d), the results obtained by dc magnetization, ac susceptibility, and ac ME coefficient are directly compared. It is seen that the skyrmion phase is consistently observed in all three thermodynamic probes. The critical magnetic fields associated with various magnetic transitions are also nicely identified.

    The magnetostriction coefficient dλ(H)/dH is directly proportional to the product of the magnetization 〈Skz〉 and the spin-spin correlation 〈Si⋅Sj〉 via the magnetoelastic coupling D(i,j):dλ(H)/dH∼∑k〈i,j〉D(i,j)〈SkzSi⋅Sj〉, making it highly sensitive to spin fluctuations.[40,41] As shown in Fig. 3(e), αx is vanishingly small well above Tc in the paramagnetic phase. Upon cooling below 330 K, αx rises rapidly, peaking at T* ∼ 312 K due to the development of spin fluctuations. In zero magnetic field, αx also diverges as it approaches T*, though with significantly smaller amplitudes compared to those in non-zero magnetic fields. The peak in αx at T* signifies the crossover between the paramagnetic state and the disordered fluctuating phase, characterized by short-range correlations, as found in MnSi.[32,42] Below T*, the establishment of short-range correlations suppresses spin fluctuations, leading to a rapid decrease in αx. Below Tc, the onset of long-range order further suppresses spin fluctuations and αx. It is noteworthy that αx changes slope at Tc [see the inset in Fig. 3(e)]. A dip appears in αx below Tc in small magnetic fields, indicating transitions between different ordered states. Note that the disordered fluctuating region between Tc and T* is not resolved in magnetization measurements [see Fig. 2(a)]. The superior sensitivity to spin fluctuations makes the magnetostriction coefficient a prominent probe for tracking complex magnetic transitions.

    Based on the ac susceptibility and ac ME data, the phase diagram of Co8Zn8Mn4 single crystals measured at ambient pressure is mapped out in Fig. 3(e). Similar phase diagrams are commonly seen in CoxZnyMnz alloys.[13,14,16,18] In zero magnetic field, a helical (H) magnetic state is formed below Tc = 309 K. In the magnetically ordered state just below Tc, applying a magnetic field between H1 and H2 drives the system into a skyrmion phase. Clearly, the skyrmion (Sk) pocket is confined in a narrow region sandwiched by a conical (C) phase in the T–H phase diagram. Moderate magnetic fields above H3 drive the system into a polarized ferromagnetic (FM) state. In addition, a disordered fluctuating (DF) region is found between the magnetic ordered state and paramagnetic (PM) state.

    Now we explore the effects of quasihydrostatic pressure on the skyrmion phase of Co8Zn8Mn4. DC magnetization measured under different pressures is shown in Figs. 4(a)–4(c). At ambient pressure (P0), the skyrmion phase is manifested as a dip in dM/dH within T ∼ 302 K–306 K and H ∼ 50 Oe–100 Oe, as also found in ac susceptibility. By applying a moderate pressure of P1 = 6.1 kbar, as presented in Fig. 4(b), the dip feature in dM/dH appears already at 310 K and persists down to 300 K. The absolute height of the dip structure is also enhanced compared to that in P0. Moreover, both the lower (H1) and upper (H2) magnetic field boundaries of the skyrmion phase are clearly increased. This trend persists to a higher pressure P2 = 9.6 kbar as shown in Fig. 4(c). Note that compared with P1, the upper temperature limit in P2 is slightly reduced back to 308 K. Figure 4(d) summarizes the phase diagram occupied by the skyrmion pocket under different pressures. Clearly, the area covered by the skyrmion phase in the T–H phase diagram is significantly enlarged under pressure. Under the pressure of P1, the absolute size of the skyrmion pocket is more than twice that at ambient pressure (P0). It has been shown that the skyrmion phase of Co8Zn8Mn4 forms a triangular equilibrium lattice at ambient pressure.[13,18,19] Our observation rules out possibilities of other topological spin textures such as magnetic meron or magnetic bubble. Magnetic meron is considered to locate between helical phase and skyrmion phase,[43] thus a pressure-induced magnetic meron would present at lower field below H1. Magnetic bubbles hold magnetic domains and own different energy scales than skyrmion,[44] thus, a pressure-induced bubble phase would monotonically evolve with increasing pressure. Furthermore, the spatial organization of skyrmions formed under pressure remains to be explored.

    Pressure-tuned expansion of the skyrmion phase has been previously observed in bulk MnSi,[22–24] Cu2OSeO3.[25,26] Since the skyrmion phase emerges near Tc, the free energy of the system can thus be described by the Ginzburg–Landau approach:[22,26]F[M]=AM2+J(∇M)2+DM⋅(∇×M)+(U+K)M4−μ0H⋅M, where the magnetization M is the order parameter, A is a temperature-dependent constant controlling Tc, J represents the ferromagnetic exchange interactions, D is the DM interaction, U describes the mode-mode interactions, and K accounts for magnetic anisotropy. Applying pressure tunes the parameters J, D, and K, which in turn manipulates the size of the skyrmion phase. Although relatively small compared to the exchange and DM interactions, magnetic anisotropy plays an essential role in stabilizing the skyrmion phase in Cu2OSeO3,[45–47]β-Mn-type CoxZnyMnz compounds,[19,48,49] and multilayer structures.[50–52] Based on the Ginzburg–Landau analysis, Levatić et al. demonstrated that the skyrmion phase is most sensitive to variations in K among the pressure-tuned parameters.[26] A moderate increase in K significantly enlarges the skyrmion phase in Cu2OSeO3,[26] while modulation of the DM interaction often leads to large deformations of the skyrmion lattice, as observed in FeGe thin plates.[53] Consequently, it is now widely accepted that pressure- or strain-induced changes in magnetic anisotropy, though small, play a crucial role in expanding the skyrmion phase.[21–26] In the case of Co8Zn8Mn4, pressure-tuned magnetic anisotropy is likely the key factor responsible for the expansion of the skyrmion phase under moderate pressure. In addition, magnetic fluctuations also play important roles in stabilizing the skyrmion phase, as found in Co7Zn7Mn6.[20] Under 6.1 kbar, the skyrmion phase of Co8Zn8Mn4 extends up to about 310 K, slightly above the Tc at ambient pressure. Stabilization of short-range correlations in the DF region under pressure may also contribute to the pressure-induced extension of the skyrmion pocket.

    Note that pressure-induced structural changes can significantly enhance the skyrmion phase, as observed in Cu2OSeO3 at high pressures of 420 kbar.[54] However, at moderate pressures, such as those in our study (below 10 kbar), significant pressure-induced structural changes are not expected. Nevertheless, pressure inhomogeneities and local strains may still occur, potentially leading to enhanced stability of the skyrmion phase.[22,55] The effects of pressure inhomogeneities or local strain on the skyrmion phase can become significant, particularly when the pressure-transmitting medium is in its solid phase.[55] For example, Levatić et al. reported pronounced pressure-induced enlargement of the skyrmion phase in Cu2OSeO3 using the pressure-transmitting medium Daphne 7373 in its solid state.[26] In contrast, negligible pressure-tuning effects on the skyrmion phase in Cu2OSeO3 were observed by Crisanti et al. using liquid helium as the pressure-transmitting medium.[55] Even in the liquid phase of helium, applied pressure imposed directional stress, slightly modulating the domain population of Cu2OSeO3.[55]

    In our study, using Daphne 7373 as the pressure-transmitting medium, pressure inhomogeneity of approximately 5% may arise at 13.4 kbar,[31] well below the solidification pressure (about 30 kbar[30]). After solidification, pressure inhomogeneities can increase up to 30%.[31] Although the effects of pressure inhomogeneities on the skyrmion phase of Co8Zn8Mn4 cannot be completely ruled out, we believe they play a subdominant role for the following reasons: (i) Since Daphne 7373 remains in its liquid phase within the temperature and pressure range studied here, moderate pressure inhomogeneities of a few percent are unlikely to significantly impact the skyrmion pocket, as also found in Cu2OSeO3;[52] (ii) Higher pressure inhomogeneity would be expected at 9.6 kbar compared to 6.1 kbar, yet the skyrmion phase shrinks in the former case. The effect of pressure inhomogeneity or directional strain on Co8Zn8Mn4 could lead to slight differences in stress on transverse and longitudinal directions, similar to the study of MnSi,[24] or weaker modulation on D relating to the complex near-EF electronic bands of Co8Zn8Mn4 compared to the modulation by strain on FeGe,[51] thus resulting in a weak shrinkage of its skyrmion pocket. On the other hand, if the remarkable enlargement of the skyrmion pocket in Co8Zn8Mn4 is indeed induced by such moderate pressure inhomogeneities or directional strain, it would be promising to explore strain-tuning of the skyrmion phase. This opens up exciting possibilities for developing skyrmion-based devices using Co8Zn8Mn4 thin films. We also note that magnetic frustrations or disorders can induce metastable skyrmion phases in CoxZnyMnz.[14,18] While magnetic frustrations or disorders are mostly arising from Mn atoms located on the 12d sites, giving rise to metastable skyrmion phases at low temperatures. The pressure-expanded skyrmion pocket near Tc found in Co8Zn8Mn4 is thus unlikely caused by magnetic frustrations or disorders.

4.   Conclusions
  • In summary, we have studied the evolution of the skyrmion phase in Co8Zn8Mn4 under quasihydrostatic pressure. It is found that the size of the skyrmion pocket on the T–H phase diagram is considerably enlarged under a moderate pressure of about 10 kbar. Although pressure inhomogeneities may exist, the enhanced stability of the skyrmion phase is likely caused by pressure-driven enhancement of magnetic anisotropy. It would be interesting to further manipulate the skyrmion phase using strain engineering on CoxZnyMnz thin films or by even higher pressure or doping to change the crystal structure of bulk CoxZnyMnz compounds.

Figure (4)  Table (1) Reference (55)

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return