2026 Volume 35 Issue 7
Article Contents

Yan Hu, Yu-Ling Song, Yu-Hong Huang, Shu-Yao Cao, Fei Ma. Structural asymmetry induced high Curie temperature and large out-of-plane piezoelectricity in Gd2COF MXenes and Gd2COF/MoS2 heterostructure[J]. Chinese Physics B, 2026, 35(7): 077102. doi: 10.1088/1674-1056/ae815f
Citation: Yan Hu, Yu-Ling Song, Yu-Hong Huang, Shu-Yao Cao, Fei Ma. Structural asymmetry induced high Curie temperature and large out-of-plane piezoelectricity in Gd2COF MXenes and Gd2COF/MoS2 heterostructure[J]. Chinese Physics B, 2026, 35(7): 077102. doi: 10.1088/1674-1056/ae815f

Structural asymmetry induced high Curie temperature and large out-of-plane piezoelectricity in Gd2COF MXenes and Gd2COF/MoS2 heterostructure

  • Received Date: 16/03/2026
    Accepted Date: 23/06/2026
    Available Online: 01/07/2026
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

Figures(7)

Article Metrics

Article views(110) PDF downloads(0) Cited by(0)

Access History

Structural asymmetry induced high Curie temperature and large out-of-plane piezoelectricity in Gd2COF MXenes and Gd2COF/MoS2 heterostructure

Abstract: Two-dimensional (2D) rare-earth (RE) ferromagnetic (FM) materials exhibit significant potential for next-generation spintronic devices. In this work, first-principles calculations are performed to study the MXene Gd2COF monolayer. We demonstrate that Gd2COF is a ferromagnetic half-metal with a large magnetic moment of 13 μB per formula unit and a Curie temperature (TC) of 750 K, the highest one among the reported RE monolayers. The high TC is attributed to both the out-of-plane structural asymmetry induced interlayer FM double-exchange interaction and the dual intralayer FM super-exchange pathways. Additionally, the system possesses a wide band gap of 3.09 eV and a magnetic anisotropy energy (MAE) of −0.25 meV, features consistent with half-metallicity and ferromagnetism. The monolayer Gd2COF is metallic with −5% ∼ −4% biaxial strain, transforms into a half-metal with −3% ∼3% biaxial strain, and then becomes a semiconductor with 4% ∼5% biaxial strain. It has a high Curie temperature of 550 K ∼ 900 K throughout the entire strain range. The Curie temperature decreases with increasing biaxial strain due to the weakened Gd–Gd and Gd–C/O/F bonds. Furthermore, the monolayer exhibits significant out-of-plane piezoelectricity at tensile strains of 4% and 5%. Furthermore, the planar Gd2COF can be stabilized when supported on monolayer MoS2 substrate to avoid bending. The Gd2COF/MoS2 heterostructure also has a high Curie temperature of 550 K ∼ 900 K with −5% ∼ 5% biaxial strain. The metal–half-metal–semiconductor transition and large piezoelectricity with strain can be similarly observed in this heterostructure.

1.   Introduction
  • Two-dimensional (2D) ferromagnetic (FM) materials possess ultrathin structure and high surface-to-volume ratio, making them promising candidates for applications in high-speed and energy-efficient devices.[1,2] 2D FM materials exhibit numerous intriguing properties, such as the proximity effect,[3,4] anomalous quantum Hall effect,[5–7] multiferroicity,[8–10] skyrmion formation[11,12] and large tunnel magnetoresistance.[13] In fact, the non-magnetic 2D systems, for example, graphene could be induced into ferromagnetism by transition metal (TM) doping, hydrogen adsorption or introduction of vacancies. However, the resulting magnetism is generally weak.[14,15] Interestingly, CrI3 monolayers[16] and bilayer Cr2Ge2Te6[17] exhibit the intrinsic ferromagnetism at the monolayer limit. The results demonstrate that the long-range magnetic order can be stabilized in two dimensions through magnetic anisotropy arising from out-of-plane structural asymmetry. Subsequently, various intrinsic 2D FM monolayers and thin films, Fe3GeTe2[18] and 1T-VSe2[19] monolayers, as well as MnS2,[20] CrTe[21] and Cr3Te4[22] thin films, were studied recently. In particular, a series of 2D FM materials, such as MX2 (M = Fe, Co, Ni; X = Cl, Br, I),[23]MX3 (M = V–Ni; X = Cl, Br, I),[24–29] CrGa2Se4,[30] MnB,[31] metal-organic frameworks (MOFs),[32]MOX (M = Cr, Mn; X = Cl, Br),[33,34] FeB3,[35] MnB6,[36] and Co2B6[37] have been theoretically investigated. Nevertheless, the Curie temperatures of most 2D FM materials are still lower than room temperature,[18,23,24,27–30,33,34,36,38–48] posing a significant challenge for the development of 2D ferromagnets suitable for practical applications.

    For TM ferromagnets, the crystal structure plays a crucial role in determining the Curie temperature. For instance, isovalent alloying can reduce the exchange gap of Cr ions in monolayer CrI3[49] and CrOX (X = Cl, Br),[50] which enhances both the virtual hopping effect and the ferromagnetic coupling, and thus significantly elevates the Curie temperature from 45 K to 180 K, from 100 K to 310 K, and from 50 K to 320 K, respectively.[49,50] Additionally, lattice strain has been demonstrated to substantially enhance the Curie temperature of 2D TM ferromagnets.[34,49] Since the real hopping from double-exchange interaction is generally stronger than the virtual hopping from super-exchange mechanisms, designing 2D FM TM materials with magnetic ions in different spin states can induce real hopping and elevate the Curie temperature, such as in monolayer Cr3X4 (X = Se, Te)[51] and Fe2X (X = S, Se).[52]

    Rare-earth (RE) elements are promising for inducing substantial magnetic moments via f-electrons,[53] and have potential applications in higher-density spintronic devices. Moreover, heavier RE ions usually exhibit stronger magnetic anisotropy due to the enhanced spin–orbit coupling (SOC), which can stabilize the magnetic order against thermal fluctuations. 2D FM RE materials, such as Gd2C,[54] EuN[55] and SmN[56] thin films, as well as Ln = X2 (Ln = Eu, Gd; X = Si, Ge) monolayers,[57] have been synthesized, in which magnetism often arises from the delocalized d-electrons, and the ferromagnetism can be mediated by the f–d–p–d–f exchange mechanism with d-electrons as intermediaries. However, this mechanism is generally weaker than the d–p hybridization effect in many 2D TM ferromagnets, so that the Curie temperatures of most 2D FM RE monolayers are still low, in the range of 17 K ∼ 281 K.[58–66] It is still a challenge to design 2D RE ferromagnets with high Curie temperatures for potential applications in RE-based spintronics.

    MXenes, a family of 2D materials with the general formula Mn+1Xn (where M is a metal and X is C or N), can be selectively functionalized with O, F, and Cl,[67] in which the multiple M layers can introduce additional interlayer FM interactions. Furthermore, inequivalent magnetic sites can be created, enabling double-exchange interactions, by constructing double-metal layers or employing asymmetric surface functionalization. This makes MXenes ideal platforms for exploring high-Curie-temperature 2D ferromagnets. It has been predicted that the asymmetric MXenes, for example, Cr2COF, Cr2COCl, Cr2CO(OH)[68] and CoMnC[69] monolayers possess high Curie temperatures of 622 K ∼ 1366 K. Moreover, similar to VSSe Janus monolayers,[70] the broken out-of-plane symmetry can induce built-in electric fields and out-of-plane piezoelectricity. Can we design asymmetric MXene-based RE monolayers with both high Curie temperature and out-of-plane piezoelectricity?

    In this work, first-principles calculations are done to investigate the stability, electronic structure, and magnetic properties of RE-based Gd2COF MXene monolayer. It is found that Gd2COF is an FM half-metal with a high Curie temperature of 750 K and a sizable magnetic anisotropy energy (MAE) of −0.25 meV per formula unit, a large band gap of 3.09 eV. The high Curie temperature can be ascribed to the broken structural symmetry-induced interlayer FM interaction and the double-exchange mechanism, since other predicted FM RE monolayers are super-exchange ferromagnets.[58–66,71–79] This value is much higher than those of other FM RE monolayers (Table S1), in particular, higher than those of monolayers T-Gd2C (322 K)[71] and Gd2B2 (550 K),[72] both of which exhibit interlayer super-exchange ferromagnetism. Under the biaxial strain of −5% ∼ 5%, Gd2COF undergoes phase transition from metal to half-metal and then semiconductor. Notably, the Curie temperature remains above room temperature (300 K) across the strain range, underscoring the robust ferromagnetism. Moreover, the asymmetric structure can induce large out-of-plane piezoelectricity. The planar Gd2COF can be stabilized when supported on monolayer MoS2 substrate to avoid bending.

2.   Computational methods
  • All the calculations are performed by spin-polarized density function theory (DFT) as implemented in the Vienna ab-initio simulation package (VASP).[80] Interactions between electrons and nuclei are described by the projector augmented wave (PAW)[81,82] and the electronic exchange–correlation interactions are described by the Perdew–Burke–Ernzerhof (PBE) functional of the generalized gradient approximation (GGA).[83] Particularly, the Hubbard U terms are adopted to calculate the strong-correlated interaction, the coulomb interaction parameter U (9.2 eV) and the exchange interaction parameter J (1.2 eV) are used to describe the behaviors of Gd-f electrons,[60,61] particularly, the Heyd–Scuseria–Ernzerh (HSE06) method with the screening parameter fixed at a value of 0.2 Å−1 was adopted to calculate the electronic band structure for comparison.[84]

    The Brillouin zone integration is carried out by 9 × 9 × 1 k-mesh based on the Monkhorst–Pack scheme.[85] The cutoff energy for the plane wave basis set is set as 500 eV. Ab-initio molecular dynamics (AIMD) simulations last for 5 ps with a time step of 2 fs in the NVT ensemble at 300 K by the Nose–Hoover method.[86] The harmonic and anharmonic phonon spectra are calculated using the Phonopy[87] and Dynaphopy codes[88] implemented within the VASP package, respectively. The convergence criterion for the total energy and force is set as 1 × 10−8 eV and 0.001 eV/Å, respectively. The crystal occupation Hamiltonian population (COHP) method employed in LOBSTER is applied to investigate the bonding and antibonding states.[89] The DFT-D3 method is employed to describe the weak dispersion forces of the van der Waals interactions for Gd2COF/MoS2 heterostructure.[90] A vacuum space of 20 Å is added along the direction perpendicular to the surface for both monolayer Gd2COF and Gd2COF/MoS2 heterostructure to avoid interactions between the adjacent periodic units.

3.   Results and discussion
  • The pristine Gd2C monolayer consists of a honeycomb lattice formed by top and bottom Gd triangular sub-layers, with C ions sandwiched between them in the space group of P-3M1 (Figs. 1(a) and 1(b)). Each Gd ion is coordinated to three nearest C ions, while each C ion is surrounded by six nearest Gd ions. On the pristine Gd2C monolayer, there are two nonequivalent adsorption sites: site A, directly above a Gd ion, and site B, below a C ion, so there are four possible configurations for Gd2COF monolayer (Figs. 1(c)–1(f)), for type-I (II) configuration, both F and O ions are located at A (B) site, while for type-III (IV) configuration, O ion is located at A (B) site but F ion is located at B (A) site. Type-I configuration is the most stable one (Table S2), suggesting a preferential hybridization between F/O and Gd ions due to the lower electronegativity of Gd ion. Based on a 2 × 1 × 1 supercell, one ferromagnetic (FM), two antiferromagnetic (AFM-1 and AFM-2), and ferrimagnetic (FiM) states are examined (Fig. S1), for the FM state, all the Gd ions are coupled ferromagnetically (Fig. S1(a)), for the AFM-1 (AFM-2) state (Figs. S1(b) and S1(c)), the nearest-neighbor (NN) intralayer (interlayer) Gd ions are coupled ferromagnetically while the NN interlayer (intralayer) Gd ions are coupled anti-ferromagnetically, for the FiM state, one Gd2 ions are coupled anti-ferromagnetically with other 3 Gd ions (Fig. S1(d)). The FM state is identified as the magnetic ground state. The optimized lattice parameters a and b are both 3.65 Å, which is close to the value of pristine Gd2C (3.62 Å).[71] After functionalization, two inequivalent Gd sites, Gd1 and Gd2, emerge. The Gd1–C and Gd1–O bond lengths are 2.80 Å and 2.22 Å, respectively, while the Gd2–C and Gd2–F bond lengths are 2.47 Å and 2.42 Å, respectively. This leads to the broken out-of-plane symmetry in the Gd2COF monolayer.

    The absorption energy is calculated using the following equation:

    where EGd2COF and EGd2C are the total energies of Gd2COF and Gd2C monolayers, EO and EF are the atomic energies of O2 and F2 gas, Δμ = μ – (1/2)E(T2), μ is the chemical potential of O and F atoms. At the temperature range of 0 K ∼ 300 K, Δμ of both O and F atoms is in the range of 0 eV ∼ −0.32 eV.[91] Accordingly, the absorption energies are in the range of −10.86 eV ∼ −10.22 eV per formula unit for the Gd2COF monolayer. The negative values confirm that the formation process remains exothermic, there are no imaginary frequencies across the Brillouin zone in the phonon spectra of Gd2COF monolayer at 0 K and 300 K, indicating dynamic stability (Figs. 2(a) and 2(b)). Moreover, AIMD simulations revealed that no bond breaking and reconstruction occur in the Gd2COF monolayer at 300 K (Fig. 2(c)), thermal oscillation of the whole structure happens near the equilibrium position, indicating good thermal stability, therefore we believe that Gd2COF monolayer can be synthesized and its structure can remain stable at room temperature.

    Finally, the independent elastic constants C11 and C12 are calculated to be 123.67 N/m and 55.48 N/m for Gd2COF monolayer, respectively. According to the isotropic lattice symmetry, the elastic constant C22 is equal to C11, and C66=12(C11−C12), thus C22 and C66 are 123.67 N/m and 34.10 N/m respectively. These elastic constants satisfy the Born–Huang stability criteria: C11 > 0, C11C22−C122>0 and C66 > 0,[92] confirming that the Gd2COF monolayer is mechanically stable. Figure 2(d) shows the calculated Young’s modulus of Gd2COF monolayer; it is isotropic with a value of 98.78 N/m, which is much larger than that of CrI3 monolayer (23.85 N/m).[93]

  • Figure 3(a) shows the spin-resolved band structures. The Gd2COF monolayer is a half-metal with an indirect band gap of 3.09 eV. It possesses a metallic spin-up channel and a semiconducting spin-down channel, with the valence band maximum (VBM) and the conduction band minimum (CBM) at −0.46 eV and 2.63 eV, respectively. According to the Fermi–Dirac distribution,[94] the thermally induced occupation probability between the valence band and the Fermi level at 300 K is on the order of 108, ensuring the stability of the half-metallic feature. As shown in Fig. 3(b), the f orbitals of both Gd1 and Gd2 ions are highly localized and far from the Fermi level. Therefore, the d–p hybridization between Gd and C/O/F ions plays a crucial role in inducing ferromagnetism. Under the C3V symmetry, the Gd-d orbitals split into dz2, e1 (dxz + dyz), and e2 (dxy + dx2 + y2) groups. The VBM is dominated by the C-px/py orbitals while the CBM is dominated by the Gd1-e1 orbitals (Fig. S2(a)). Moreover, the hybridizations between Gd1/Gd2 and C ions are stronger than those between Gd1–O/Gd2–F ions. The spin-up and spin-down channels of O and F-p orbitals are almost fully occupied (Fig. S2(b)), corresponding to the valence electron configurations of 2s2p6 for O and F ions, while the spin-up channel of C-p orbitals is partially occupied. Moreover, at the HSE06 level, the Gd2COF monolayer is also a FM half-metal (Fig. S2(c)). According to the Bader analysis (Table S3), Gd1 and Gd2 ions donate 1.62 and 1.72 electrons to C ions, respectively, while O and F ions acquire 1.87 and 0.92 electrons from them, respectively. This results in a magnetic moment of 6/7 μB for Gd1/Gd2 ions but a negligible one on C, O, and F ions. The AFM-1 state converted to the FiM-1 state as well. To explain the origin of the electron transfer mechanism, we calculated the electron localization function (ELF) (Fig. S3). The values of ELF for the regions between Gd and C/O/F ions range from 0 to 0.25, reflecting the nature of Gd–C/O/F ionic bonding. Therefore, Gd ions can donate more electrons to C/O/F ions. In addition, more charge accumulates between the Gd and C ions, indicating that both Gd1–C and Gd2–C bonds have more covalent character than Gd1–O and Gd2—F bonds.

    The magnetic ground state of Gd2COF is governed by the interplay between the direct and indirect exchange interactions among Gd ions. The direct exchange interaction, mediated primarily by the nearly half-filled Gd-f orbitals, exhibits FM coupling between neighboring Gd ions, consistent with Hund’s rule.[95] Simultaneously, the indirect exchange interaction arises from d–p hybridization between Gd ions and the surrounding C, O and F ions. According to the Goodenough–Kanamori–Anderson (GKA) rule,[96] when the bond angle between two Gd ions via a nonmagnetic ligand is close to 90°, the Gd-d orbitals tend to hybridize with orthogonal p orbitals of the C, O and F ions, leading to FM coupling between Gd ions according to the symmetry (Fig. S4(a)). As illustrated in Fig. 3(c), the calculated θ1, θ2, θ3 and θ4 are 91.3°, 81.2°, 110.6° and 98.0°, respectively, suggesting the existence of FM indirect exchange between both nearest-neighbor intralayer and interlayer Gd ions.

    The magneto-crystalline anisotropy energy (MCE) is defined as the differences between the in-plane and out-of-plane magnetization directions, as EMCE = Ez – Ex/y, where Ez and Ex(y) denote the total energies when magnetization is aligned along z and x (y) axes, respectively. For Gd2COF monolayer, the calculated MCE is −1.37 meV per formula unit, the negative value indicates that the easy magnetization axis is out-of-plane oriented. Given the large magnetic moment of Gd ions, we further calculated the magnetic dipolar energy (MDE) for Gd2COF monolayer. For a FM system, the MDE in atomic Rydberg units is given by[97]

    where the speed of light c = 137.036 a.u., i/j are the atomic position vectors in the unit cell, and mi/mj is the atomic magnetic moment on sites i/j (in units of μB). The magnetic dipolar Madelung constant Mij is calculated as

    where R are the lattice vectors. The shape anisotropy energy ΔEd (SAE) is calculated to be 0.474 meV and 0.646 meV for Gd1 and Gd2 ions, respectively, yielding a total SAE of 1.12 meV per formula unit of Gd2COF, because the magnetostatic dipole–dipole interactions weaken the out-of-plane magnetic anisotropy. The net magnetic anisotropy energy (MAE) of Gd2COF monolayer is −0.25 meV per formula unit, although this value is considerably smaller than the MCE, it remains notably larger than the MAE of bulk Fe (0.001 meV/atom)[98] and Ni (0.003 meV/atom),[98] such the MAE is sufficient to stabilize the long-range magnetic order in the Gd2COF monolayer.

    The magnetic exchange interactions between nearest-neighbor (NN) interlayer and intralayer Gd ions are described by the parameters J1, J2 and J3 (Fig. 3(c)). The spin Hamiltonian is expressed as[99]

    where J1, J2 and J3 are the exchange coupling parameters, M is the net magnetic moment of Gd ions, i and j (k and l, m and n) stand for the interlayer (intralayer) nearest neighboring Gd ions, A is the magnetic anisotropy parameter, Miz represents net magnetic moment per formula unit along a preferred axis and A(Miz)2 is the total MCE. Correspondingly, the total energies of FM, AFM, FiM-1 and FiM-2 states in the 2 × 1 × 1 supercell can be expressed as

    The magnetic coupling parameters are derived from energy differences between FM and the other states:

    The calculated J1, J2 and J3 are 0.86 meV, 1.04 meV and 0.43 meV, respectively. The positive values indicate a preference for FM coupling. The Curie temperature (TC) of the Gd2COF monolayer is evaluated using statistical Monte Carlo (MC) simulations based on the Heisenberg model. A 100 × 100 × 1 supercell containing 20000 magnetic moment vectors is employed, which lasts for 105 MC steps at each temperature. Magnetic moments are randomly rotated at each step. We estimated the TC value of 42 K for CrI3 monolayer,[98] in good agreement with the experimental value.[16] The results confirm the accuracy of the calculation method. As shown in Fig. 3(d), the specific heat CV is defined as CV = (〈E2〉 – 〈E〉2)/(kBT2). The peak value of CV corresponds to TC of 750 K for Gd2COF monolayer, which is higher than the TC of other predicted 2D FM RE monolayers,[58–66,71–79] which range from 17 K to 648 K (Table S1). Apparently, the Gd2COF monolayer possesses the highest TC among all the predicted FM RE monolayers. Owing to the distinct spin states of Gd1 and Gd2 ions, the indirect interlayer coupling between the nearest-neighbor Gd ions is attributed to the double-exchange mechanism. As illustrated in Fig. S4(b), in this case ferromagnetism originates from interactions between the highest occupied Gd2-d orbital and the lowest unoccupied Gd1-d orbital based on the Pauli exclusion principle. The distinct spin states of Gd1 and Gd2 ions typically exhibit a smaller exchange d–d gap; thus the double-exchange mechanism driven by real electron hopping is beneficial to both FM coupling and high Curie temperature. In contrast, the indirect intralayer interactions between neighboring Gd1 (or Gd2) ions are governed by the super-exchange interaction, while in this case interactions between the highest occupied Gd1-d (Gd2-d) orbital and the lowest unoccupied Gd1-d (Gd2-d) orbital induce ferromagnetism (Fig. S4(c)). The virtual electron hopping brings a larger exchange d–d gap, which is unfavorable for FM coupling. But in addition to the Gd1–C–Gd1 (and Gd2–C–Gd2) pathways, super-exchange interaction between intralayer Gd1 (or Gd2) ions can also be mediated through Gd1–O–Gd1 (and Gd2–F–Gd2) routes. The multiple super-exchange pathways further enhance the overall FM coupling. The double-exchange interlayer coupling and the multi-path super-exchange intralayer interactions lead to robust FM ordering among Gd ions and high Curie temperature. At 750 K, monolayer Gd2COF can also maintain dynamic and thermal stability (Fig. S5).

  • Commonly, the Gd2COF monolayer tends to bend along the out-of-plane direction. In a 3 × 2 × 1 supercell model with a bending radius of 3.72 Å (Fig. 4(b)), the curved nanotube configuration exhibits the lowest energy, being more stable than the planar Gd2COF monolayer by 0.008 eV/Å2 (Figs. 4(c) and 4(d)). However, the planar Gd2COF can be stabilized when supported on a monolayer MoS2 substrate (Fig. S6), since the interfacial binding energy exceeds −0.008 eV/Å2 (−0.024 eV/Å2); the flat surface electrostatic potential in the regions on both sides of the heterojunction shows that the vacuum space is thick enough (Fig. S7). Moreover, the substrate can also induce biaxial strain which can modulate the electronic and magnetic properties[72] effectively. In this work, we systematically investigated the electronic and magnetic properties of the Gd2COF monolayer under biaxial strain of −5% ∼ +5%. It is found that the Gd2COF monolayer maintains an FM ground state. The magnetic moments of Gd1 and Gd2 ions remain 6 μB and 7 μB, respectively, but those of C, O, and F ions remain negligible. Consequently, the double-exchange interlayer coupling and the multi-path super-exchange intralayer interactions remain unchanged. Gd2COF monolayer undergoes a phase transition from metal to half-metal and then to semiconductor (Fig. 5).

    Under the compressive strain of −5% ∼ −4%, the electronic states from both spin-up and spin-down channels cross the Fermi level, characteristic of a FM metal. Under the strains of −3% and +3%, the monolayer exhibits a robust half-metallic state: the spin-down channel has a band gap of about 3.05 eV, while the spin-up channel remains metallic. Under the strains below +1%, the VBM increases firstly, and then decreases slightly, but the CBM changes in an opposite trend, the maximum VBM and CBM are 0.50 eV and 2.94 eV at the strains of +1% and −3%, respectively. At the larger tensile strains of 4% ∼ 5%, Gd2COF monolayer transforms into a FM semiconductor, with both spin channels possess band gaps, in which the VBM and CBM are dominated by the spin-up channel with a band gap of 1.95 eV. At a strain of 4%, the VBM is only 0.15 eV below the Fermi level, leading to a thermally induced valence–Fermi level occupation probability on the magnitude order of 10−3 at 300 K (Fig. 6(a)).

    With increasing strain, band structures move downwards overall because of weaker Coulomb repulsion, leading to phase transition from metal to half-metal and then to semiconductor. For both spin channels, occupied C-px/py orbitals have less weight in the highest occupied energy band, while unoccupied Gd1-e1 and e2 orbitals have more weight in the lowest unoccupied energy band, indicating these orbitals are also more sensitive to the in-plane biaxial strain and thus tend to move downwards with increasing strain correspondingly (Fig. S8). On the other hand, under compressive strain, interactions between Gd-d and C-p orbitals become stronger, which makes both Gd-d and C-p orbitals more delocalized (Fig. S9). In the spin-up channel, a more delocalized highest occupied energy band crosses the Fermi level, resulting in half-metallicity. In contrast, under tensile strain, weaker interactions between Gd-d and C-p orbitals make these orbitals become more localized (Fig. S9); thus, in the spin-up channel, they become far from the Fermi level, and at −4% and −5% strain, both spin channels are semiconducting. Compared with Gd2-d orbitals, hybridizations between Gd1-d and C-p orbitals are more sensitive to the biaxial strain.

    Considering the effect of substrate, under biaxial strain of −5% ∼ −2%, the heterostructure is an FM metal, while it converts to a half-metal under biaxial strain of −1% ∼ 3%. With biaxial strains of 4% ∼ 5%, it is still an FM semiconductor, and the magnetic moments of Gd1 and Gd2 ions remain unchanged throughout this strain range (Fig. S10).

    Moreover, the structural asymmetry along the z-axis gives rise to out-of-plane piezoelectricity with the piezoelectric coefficient e31 of 56.3 pC/m and 78.2 pC/m in the Gd2COF monolayer under a biaxial strain of 4% and 5%, respectively. This value is much larger than those of monolayers Janus MXY (M = Mo, W; X/Y = S, Se, Te) (1 ∼ 3.8 pC/m),[100] comparable to those of monolayer Y2CO2 (88 pC/m),[101] In2Se3 (51.7 pC/m),[102] yet smaller than those of Sc2CO2 (196 pC/m) and La2CO2 (120 pC/m),[101] in comparison with other FM monolayers, this value is much larger than those of CrSI (2 pC/m),[103] VSeTe (11 pC/m),[104] and VSTe (36 pC/m),[104] comparable to that of CrSBr (71 pC/m),[103] smaller than that of CrSCl (121 pC/m).[103] Since there have been no reports so far on the piezoelectricity of 2D FM RE materials, monolayer Gd2COF would be a research hotspot in the field of RE piezoelectric ferromagnetism.

    Consistent with M2CO2 (M = Sc, Y, La) monolayers,[101] the in-plane piezoelectric coefficients e11 of Gd2COF, 287.3 pC/m and 354.2 pC/m at strains of 4% and 5%, are significantly larger than its out-of-plane coefficients. Moreover, both e11 and e31 for Gd2COF/MoS2 heterostructure at 4%/5% strain are 328.6/376.3 pC/m and 68.2/83.8 pC/m, respectively, indicating the piezoelectricity of Gd2COF monolayer can be reinforced by the MoS2 substrate.

    Under the biaxial strains of −5% ∼ 5%, the magnetic exchange parameters J1, J2, and J3 all decrease monotonically with increasing strain (Fig. 6(b)). Firstly, the direct FM exchange between Gd ions is weakened, because the Gd–Gd bond length is elongated under tensile strain. Secondly, quantitative descriptions of bonding characteristics by the COHP analyses are given in Fig. S11. The positive/negative values of –COHP denote the bonding/anti-bonding states; thus, both the Gd–C and Gd–O/F bonds are weakened under the tensile strain, which reduces the indirect FM exchange interactions and lowers the Curie temperature. The values of integrated orbital-projected –COHP (–IpCOHP) for both Gd1–O (0.058) and Gd2–F (0.017) bonds are close to zero (Fig. S11), indicating their stronger ionic bonding characteristic, which originates from the great differences in electronegativity between Gd (1.2) and O (3.44)/F (3.98) elements, while the larger values of –IpCOHP for both Gd1–C and Gd2–C bonds indicate these bonds have a more covalent tendency, which is in agreement with our previous analysis of the ELF. Moreover, compared with Gd1–C bond, the smaller value of –COHP for Gd2–C bond is probably due to its stronger ionic bonding feature, even though the Gd2–C bond length is shorter. Throughout this strain range, the values of –IpCOHP for all specified interactions are still small, indicating all these bonds are still ionic.

    Across the strain range of −4% ∼ 5%, J2 remains the largest one among the three parameters, attributable to the stronger super-exchange interactions along both Gd1–C–Gd1 and Gd1–O–Gd1 pathways. Although the interlayer nearest-neighbor Gd ions are mediated only by the Gd1–C–Gd2 exchange path, J1 remains greater than J3 due to the dominant role of the double-exchange mechanism. At a strain of −5%, J1 and J2 are nearly equal, the Curie temperature of the Gd2COF monolayer decreases with increasing biaxial strain, from 900 K at −5% to 550 K at 5%, but remains above room temperature across the entire strain range (Figs. 7(a) and 7(b)). After considering the substrate effect, the J1, J2, and J3 remain nearly unchanged throughout this strain range, positive values for J1, J2, and J3 indicate a preference for FM coupling for both interlayer and intralayer NN Gd ions, the simulated Curie temperature for the Gd2COF/MoS2 heterostructure also remains unchanged (Fig. S12), except at −1%/4% strain which the Curie temperature increased/decreased slightly to 760 K/580 K, respectively.

    Throughout this strain range, the easy magnetization axis remains perpendicular to the xy-plane. The MCE reaches a maximum value of 1.62 meV at a strain of 4% (Fig. 6(c)). It decreases from 1.53 meV to 1.31 meV as the strain is changed from −5% to 2%, then increases at a strain of 4%, but decreases to 1.37 meV at a strain of 5%. In contrast, the SAE consistently favors in-plane magnetization. The magnitude of SAE decreases with increasing strain due to the enlarged R. Since the SAE contribution opposes that of MCE, the inclusion of SAE weakens the overall out-of-plane magnetic anisotropy. Nevertheless, the net MAE maintains the same easy axis direction as the MCE, with values ranging from 0.22 meV to 0.61 meV across the applied strain range.

4.   Conclusion
  • In summary, we designed an asymmetric MXene monolayer Gd2COF to modulate both interlayer FM and double-exchange interactions, for which the stability, electronic structure, and magnetic properties of Gd2COF monolayer have been systematically investigated. Our findings demonstrate that Gd2COF is an FM half-metal with a Curie temperature of 750 K, a spin-down band gap of 3.09 eV, and a significant out-of-plane MAE of −0.25 meV per formula unit, possessing the highest Curie temperature among the predicted 2D FM RE monolayers. The total magnetic moment is 13 μB per formula unit, predominantly contributed by the Gd ions. Under a biaxial strain of −5% ∼ 5%, the system undergoes a phase transition from metal to half-metal and then to semiconductor. The Curie temperature decreases from 900 K to 550 K, as the biaxial strain is increased. This can be ascribed to the weakened direct and indirect FM exchange interactions, as a result of the elongated Gd–Gd bonds and the softened Gd–C/O/F bonds, respectively. The easy magnetization axis remains out-of-plane across the entire strain range. Furthermore, notable out-of-plane piezoelectricity is observed under tensile biaxial strains of 4% and 5%. More importantly, the planar Gd2COF can be stabilized when supported on monolayer MoS2 substrate to avoid bending, and the Gd2COF/MoS2 heterostructure also has a high Curie temperature of 550 K ∼ 900 K with −5% ∼ 5% biaxial strain. The metal–half-metal–semiconductor transition and large piezoelectricity with strain can be similarly observed in this heterostructure.

Figure (7)  Reference (104)