Long Chengde, Zhao Bin, Yuan Peng, Hu Guangyue, Zheng Jian. 2014: Simulation of expansion of aluminum plasmas produced by a small focal spot nanosecond laser irradiation, High Power Lase and Particle Beams, null(10): 185-190. doi: 10.11884/HPLPB201426.102005
Citation: Long Chengde, Zhao Bin, Yuan Peng, Hu Guangyue, Zheng Jian. 2014: Simulation of expansion of aluminum plasmas produced by a small focal spot nanosecond laser irradiation, High Power Lase and Particle Beams, null(10): 185-190. doi: 10.11884/HPLPB201426.102005

小焦斑纳秒激光烧蚀铝平面靶的数值研究

Simulation of expansion of aluminum plasmas produced by a small focal spot nanosecond laser irradiation

  • 摘要: 用二维辐射流体程序 Flash模拟了小焦斑纳秒激光与铝平面靶的相互作用过程,其中入射激光的聚焦半径为25μm,峰值强度约为1013 W/cm2,波长为532 nm。模拟发现激光通道上的等离子体出现了密度排空的现象,激光焦斑外侧出现环状的射流结构。激光通道上密度排空现象对电子热输运的计算较为敏感,对比干涉实验测量的密度分布,确定了模拟中限流因子的取值为0.08。通过考察辐射致冷与电子横向热输运对等离子体膨胀运动的影响,对环状射流结构的形成原因给出了物理解释,并在模拟上验证了辐射冷却在其形成过程中的主导作用。
  • 加载中
  • 加载中
计量
  • 文章访问数:  294
  • HTML全文浏览数:  83
  • PDF下载数:  19
  • 施引文献:  0
出版历程
  • 刊出日期:  2014-10-30

小焦斑纳秒激光烧蚀铝平面靶的数值研究

  • 中国科学技术大学 近代物理系,合肥 230026; 中国科学技术大学 中国科学院近地空间环境重点实验室,合肥 230026

摘要: 用二维辐射流体程序 Flash模拟了小焦斑纳秒激光与铝平面靶的相互作用过程,其中入射激光的聚焦半径为25μm,峰值强度约为1013 W/cm2,波长为532 nm。模拟发现激光通道上的等离子体出现了密度排空的现象,激光焦斑外侧出现环状的射流结构。激光通道上密度排空现象对电子热输运的计算较为敏感,对比干涉实验测量的密度分布,确定了模拟中限流因子的取值为0.08。通过考察辐射致冷与电子横向热输运对等离子体膨胀运动的影响,对环状射流结构的形成原因给出了物理解释,并在模拟上验证了辐射冷却在其形成过程中的主导作用。