La2-xNdxCuO4+δ(0.1≤x≤1.2)体系中滞弹性弛豫与相变内耗研究

上一篇

下一篇

何庆, 杨春利, 吴修胜, 陈志军, 陈初升, 刘卫. 2010: La2-xNdxCuO4+δ(0.1≤x≤1.2)体系中滞弹性弛豫与相变内耗研究, 物理学报, 59(11): 7979-7985.
引用本文: 何庆, 杨春利, 吴修胜, 陈志军, 陈初升, 刘卫. 2010: La2-xNdxCuO4+δ(0.1≤x≤1.2)体系中滞弹性弛豫与相变内耗研究, 物理学报, 59(11): 7979-7985.
He Qing, Yang Chun-Li, Wu Xiu-Sheng, Chen Zhi-Jun, Chen Chu-Sheng, Liu Wei. 2010: Anelastic relaxation and phase transition internal friction properties of La2-xNdxCuO4+δ(0.1≤x≤1.2)compounds, Acta Physica Sinica, 59(11): 7979-7985.
Citation: He Qing, Yang Chun-Li, Wu Xiu-Sheng, Chen Zhi-Jun, Chen Chu-Sheng, Liu Wei. 2010: Anelastic relaxation and phase transition internal friction properties of La2-xNdxCuO4+δ(0.1≤x≤1.2)compounds, Acta Physica Sinica, 59(11): 7979-7985.

La2-xNdxCuO4+δ(0.1≤x≤1.2)体系中滞弹性弛豫与相变内耗研究

Anelastic relaxation and phase transition internal friction properties of La2-xNdxCuO4+δ(0.1≤x≤1.2)compounds

  • 摘要: 通过对La2-xNdxCuO4+δ(0.1≤x≤1.2)体系中滞弹性弛豫与相变内耗性能的研究发现,当0.1≤x≤1.0时,在250K左右存在一个与间隙氧有关的弛豫内耗峰,并且当0.1≤x≤0.4时,弛豫内耗峰峰高随着x值的增大而升高,此时体系为正交结构;当0.5≤x≤1.0时,体系在宏观上呈现四方结构,此时内耗峰峰高随着x值的增大而降低,当x继续增大到1.2时,内耗峰完全消失.此外,在0.1≤x≤0.8区间,高温区550 K左右还存在一个相变内耗峰,其相转变温度随着x值的增大向高温偏移,相应温区的弹性模量有异常变化.分析表明,此相变峰对应着体系中的正交一四方相的转变.
  • 加载中
  • 加载中
计量
  • 文章访问数:  324
  • HTML全文浏览数:  41
  • PDF下载数:  0
  • 施引文献:  0
出版历程
  • 刊出日期:  2010-11-30

La2-xNdxCuO4+δ(0.1≤x≤1.2)体系中滞弹性弛豫与相变内耗研究

  • 中国科学技术大学先进功能材料与器件实验室,合肥,230026
  • 安徽建筑工业学院先进建筑材料安徽省重点实验室,合肥,230022

摘要: 通过对La2-xNdxCuO4+δ(0.1≤x≤1.2)体系中滞弹性弛豫与相变内耗性能的研究发现,当0.1≤x≤1.0时,在250K左右存在一个与间隙氧有关的弛豫内耗峰,并且当0.1≤x≤0.4时,弛豫内耗峰峰高随着x值的增大而升高,此时体系为正交结构;当0.5≤x≤1.0时,体系在宏观上呈现四方结构,此时内耗峰峰高随着x值的增大而降低,当x继续增大到1.2时,内耗峰完全消失.此外,在0.1≤x≤0.8区间,高温区550 K左右还存在一个相变内耗峰,其相转变温度随着x值的增大向高温偏移,相应温区的弹性模量有异常变化.分析表明,此相变峰对应着体系中的正交一四方相的转变.