AA 2037新型连铸铝合金热轧板退火的正电子湮没研究

上一篇

下一篇

吴世亮, 陈叶清, 吴奕初, 王少阶, 温熙宇, 翟同广. 2006: AA 2037新型连铸铝合金热轧板退火的正电子湮没研究, 物理学报, 55(11): 6129-6135. doi: 10.3321/j.issn:1000-3290.2006.11.093
引用本文: 吴世亮, 陈叶清, 吴奕初, 王少阶, 温熙宇, 翟同广. 2006: AA 2037新型连铸铝合金热轧板退火的正电子湮没研究, 物理学报, 55(11): 6129-6135. doi: 10.3321/j.issn:1000-3290.2006.11.093
Wu Shi-Liang, Chen Ye-Qing, Wu Yi-Chu, Wang Shao-Jie, Wen Xi-Yu, Zhai Tong-Guang. 2006: Positron annihilation study of hot band of a continuous cast AA 2037 Al alloy after annealing, Acta Physica Sinica, 55(11): 6129-6135. doi: 10.3321/j.issn:1000-3290.2006.11.093
Citation: Wu Shi-Liang, Chen Ye-Qing, Wu Yi-Chu, Wang Shao-Jie, Wen Xi-Yu, Zhai Tong-Guang. 2006: Positron annihilation study of hot band of a continuous cast AA 2037 Al alloy after annealing, Acta Physica Sinica, 55(11): 6129-6135. doi: 10.3321/j.issn:1000-3290.2006.11.093

AA 2037新型连铸铝合金热轧板退火的正电子湮没研究

Positron annihilation study of hot band of a continuous cast AA 2037 Al alloy after annealing

  • 摘要: 应用正电子湮没等技术对AA 2037连铸铝合金热轧板不同温度退火下空位-溶质相互作用及沉淀相进行了研究,研究表明:室温时效形成的主要是空位-铜复合体以及空位-镁-铜复合体;温度为200℃退火时由于过渡相的形成正电子平均寿命出现峰值,符合多普勒展宽谱的商谱中观察到锰信号的存在,表明形成了空位-镁-锰复合体或过渡相中可能存在锰;温度高于250℃时,随着过渡相变粗、溶解,锰信号消失,而铜信号增强,在350℃后铜信号达到饱和,温度为450℃左右时,稳定相形成.
  • 加载中
  • 加载中
计量
  • 文章访问数:  547
  • HTML全文浏览数:  157
  • PDF下载数:  60
  • 施引文献:  0
出版历程
  • 刊出日期:  2006-11-30

AA 2037新型连铸铝合金热轧板退火的正电子湮没研究

  • 武汉大学物理科学与技术学院,武汉,430072
  • 燕山大学材料工程学院,河北秦皇岛,066002
  • Chemical and Materials Engineering Department,University of Kentucky,Lexington,KY 40506-0046,USA

摘要: 应用正电子湮没等技术对AA 2037连铸铝合金热轧板不同温度退火下空位-溶质相互作用及沉淀相进行了研究,研究表明:室温时效形成的主要是空位-铜复合体以及空位-镁-铜复合体;温度为200℃退火时由于过渡相的形成正电子平均寿命出现峰值,符合多普勒展宽谱的商谱中观察到锰信号的存在,表明形成了空位-镁-锰复合体或过渡相中可能存在锰;温度高于250℃时,随着过渡相变粗、溶解,锰信号消失,而铜信号增强,在350℃后铜信号达到饱和,温度为450℃左右时,稳定相形成.

English Abstract

参考文献 (0)

目录

/

返回文章
返回